Exploring ultrafast single-photon emission of silicon-vacancy color centers in diamond nano-membranes coupled with gold nano-cones
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-09-03 |
| Authors | Haritha Kambalathmana, Assegid M. Flatae, S. Lagomarsino, Hossam Galal, Francesco Tantussi |
| Institutions | Istituto Nazionale di Fisica Nucleare, Sezione di Firenze, University of Florence |
| Citations | 4 |
Abstract
Section titled āAbstractāSilicon-vacancy (SiV) color centers in diamond offer novel possibilities to probe light-matter interaction in nano-quantum optics and provide a scalable quantum system suitable for single-photon emission. However, their effective count-rate is still limited by non-radiative decay channels, radiation at wide angles and total internal reflection at the diamond interface. Recently optical antennas have been utilized in order to modify light-matter interaction at the nanoscale. Acting as resonators, they are able to increase the spontaneous emission rate of quantum emitters by several orders of magnitude in a broad spectral range. Because coupling a quantum emitter to a nano-Antenna requires close proximity between the two systems, we implant Si ions on very thin diamond membranes that provide the required dimension for near-field interaction in a controlled manner and investigate the optical properties of SiV color centers in such diamond membranes. We consider gold nano-cones as nano-Antennas, fabricated by focused electron beam induced deposition (EBID), followed by sputtering and focused ion beam (FIB) milling. The finite-difference time-domain (FDTD) calculations show that gold nano-cones can provide more than four orders of magnitude enhancement in the Purcell factor with an antenna efficiency (AE) of 80%.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2005 - Single-photon sources Related content Engineered quantum dot single-photon sources
- 1994 - Silicon defects in diamond