Investigation of High Voltage Anodic Plasma (HVAP) Ag-DLC Coatings on Ti50Zr with Different Ag Amounts
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2019-11-26 |
| Journal | Coatings |
| Authors | Andrei Bogdan Stoian, Cristina Surdu-Bob, A. Anghel, Daniela IoniČÄ, Ioana Demetrescu |
| Institutions | National Institute for Laser Plasma and Radiation Physics, Academy of Romanian Scientists |
| Citations | 5 |
Abstract
Section titled āAbstractāThe paper presents the investigation of a series of silver-incorporated diamond-like carbon (Ag-DLC) coatings with increasing Ag content on Ti50Zr and deposited using high voltage anodic plasma (HVAP). The coatings surface properties were analyzed with scanning electron microscope (SEM), atomic force microscope (AFM), and contact angle determinations. Electrochemical tests were performed in Afnor artificial saliva and evaluated by potentiodynamic polarization and electrochemical impedance spectroscopy. Based on these properties, comparisons of coatings performance were linked with the amount of deposited Ag. Increasing the Ag content led to the increase of the corrosion resistance and to the decrease of the forces exhibited on the surface. The hydrophobic character of the coating with the highest Ag amount could prevent thrombosis, thus suggesting its possible use for medical implants.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2011 - Modifying the TiAlZr biomaterial surface with coating, for a better anticorrosive and antibacterial performance [Crossref]
- 2009 - The binary (TiZr) alloyāA newly developed (Ti) alloy for use in dental implant
- 2017 - Binary titanium alloys as dental implant materialsāA review [Crossref]
- 2012 - A review of titanium zirconium (TiZr) alloys for use in endosseous dental implants [Crossref]
- 2018 - Corrosion and antibacterial characterization of Ag-DLC coatingon a new CoCrNbMoZr dental alloy [Crossref]
- 2018 - Silver doped diamond-like carbon antibacterial and corrosion resistance coatings on titanium [Crossref]
- 2014 - Electrochemical behaviour of ZrTi alloys in artificial physiological solution simulating in vitro inflammatory conditions [Crossref]
- 2018 - Evaluation of corrosion resistance of implant-use Ti-Zr binary alloys with a range of compositions [Crossref]
- 2013 - Tensile strength of (Zr-Ti) binary alloy [Crossref]