Star-Shaped Diketopyrrolopyrrole–Zinc Porphyrin that Delivers 900 nm Emission in Light-Emitting Electrochemical Cells
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-11-08 |
| Journal | Chemistry of Materials |
| Authors | Mariza Mone, Shi Tang, Petri Murto, Birhan A. Abdulahi, Christian Larsen |
| Institutions | Addis Ababa University, Zhengzhou University |
| Citations | 42 |
Abstract
Section titled “Abstract”The development and application of a deep near-infrared (NIR) emitting star-shaped diketopyrrolopyrrole-Zn-porphyrin compound, ZnP(TDPP)4, is reported. The structure, conjugation, and planarity of the porphyrin compound were carefully tuned by molecular design, which resulted in a low-energy photoluminescence peak at 872 nm. The ZnP(TDPP)4 compound was employed as the emissive guest in light-emitting electrochemical cells (LECs), which also comprised the conjugated polymer poly[1,3-bis(2-ethylhexyl)-5-(5-(6-methyl-4,8-bis(5-(tributylsilyl)thiophen-2-yl)benzo[1,2-b:4,5-b′]dithiophen-2-yl)thiophen-2-yl)-7-(5-methylthiophen-2-yl)-4H,8H-benzo[1,2-c:4,5-c′]dithiophene-4,8-dione] (PBDTSi-BDD) as the majority host, an ionic liquid as the electrolyte, and two air-stabile electrodes. These systematically optimized host-guest LECs featured a peak electroluminescence at 900 nm, which was delivered at a significant radiance of 36 μW/cm2 and at a low drive voltage of 3.8 V. It is notable that this is the most redshifted NIR emission attained from an LEC device to date, and as such, this work introduces Zn porphyrins as a sustainable and tunable option for emerging emissive NIR applications.