Analysis of the charge state of nitrogen-vacancy centers in diamond driven by an infrared laser field

MetadataDetails
Publication Date2019-12-01
JournalJournal of Physics Conference Series
AuthorsM. A. Smirnov, И. В. Федотов, S. A. Moiseev, А. М. Желтиков
InstitutionsRussian Quantum Center, Texas A&M University

The methods of controlling the charge state of nitrogen-vacancy centers using pulsed infrared laser field are studied. The effect of radiation intensity at a wavelength of about 1 μm on the ionization of these color centers was shown. The obtained results can be useful for multiphoton microscopy of biological objects, high-resolution microscopy and sensory applications.