Comparison of Composite Laminates Machining Methods and its Influence on Process Temperature and Edge Quality
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2019-12-01 |
| Journal | Transactions of the Institute of Aviation |
| Authors | Robert JaĹkiewicz |
| Institutions | Ĺukasiewicz Research Network, Ĺukasiewicz Research Network - Institute of Aviation |
| Citations | 2 |
Abstract
Section titled âAbstractâAbstract The article presents the description of technological trials and the results of three methods of machining carbon fiber reinforced composites panels. It also reviews the literature concerned heat affected zone in composites and its influence on material properties. As a part of the research, the cutting method using diamond coated saw was tested, as well as the milling method with two different types of carbide milling cutters. The processing of the panels was done using 4-axis CNC machine with special adapter for cutting discs in Composite Testing Laboratory (Center for Composite Technologies, Warsaw Institute of Aviation). The methods were compared in terms of machined edge quality and panel temperature during the processes. For this purpose, thermocouples were mounted into panels. Records from thermocouples were included. Edge quality and surface roughness have been checked by microscopic observation. Additionally, samples machined by each evaluated processing method were tested using differential scanning calorimetry (DSC). The method was used to determine the glass transition temperature of the tested material. The article conclusions contain a comparison of three processing methods in terms of cutting quality, process temperature, processing method productivity as well as DSC tests results.