Coupling Silicon Vacancies in Diamond to a Silica Microsphere Optical Resonator
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Journal | Frontiers in Optics / Laser Science |
| Authors | Abigail Pauls, Ignas Lekavicius, Hailin Wang |
| Institutions | University of Oregon |
| Citations | 1 |
Abstract
Section titled āAbstractāWe report the development of a composite system for cavity QED studies of silicon vacancies in diamond utilizing an ultra thin diamond membrane coupled to a silica microsphere optical resonator with < 40 MHz cavity linewidths.