Diamond Sodium Guide Star Laser
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-01-01 |
| Authors | Xuezong Yang, OndÅej Kitzler, David J. Spence, Zhenxu Bai, Yan Feng |
| Institutions | Shanghai Institute of Optics and Fine Mechanics, Hebei University of Technology |
Abstract
Section titled āAbstractāFor the first time, a 22 W continuous-wave sodium guide star laser is demonstrated in an external standing-wave diamond Raman resonator with intra-cavity second harmonic generation.