Engineering Electron–Phonon Coupling of Quantum Defects to a Semiconfocal Acoustic Resonator
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2019-09-09 |
| Journal | Nano Letters |
| Authors | H. Y. Chen, Noah Opondo, Boyang Jiang, E. R. MacQuarrie, Raphaël S. Daveau |
| Institutions | Cornell University, Purdue University West Lafayette |
| Citations | 42 |
Abstract
Section titled “Abstract”Diamond-based microelectromechanical systems (MEMS) enable direct coupling between the quantum states of nitrogen-vacancy (NV) centers and the phonon modes of a mechanical resonator. One example, a diamond high-overtone bulk acoustic resonator (HBAR), features an integrated piezoelectric transducer and supports high-quality factor resonance modes into the gigahertz frequency range. The acoustic modes allow mechanical manipulation of deeply embedded NV centers with long spin and orbital coherence times. Unfortunately, the spin-phonon coupling rate is limited by the large resonator size, >100 μm, and thus strongly coupled NV electron-phonon interactions remain out of reach in current diamond BAR devices. Here, we report the design and fabrication of a semiconfocal HBAR (SCHBAR) device on diamond (silicon carbide) with <i>f</i> × <i>Q</i> > 10<sup>12</sup> (>10<sup>13</sup>). The semiconfocal geometry confines the phonon mode laterally below 10 μm. This drastic reduction in modal volume enhances defect center coupling to a mechanical mode by 1000 times compared to prior HBAR devices. For the native NV centers inside the diamond device, we demonstrate mechanically driven spin transitions and show a high strain-driving efficiency with a Rabi frequency of (2π)2.19(14) MHz/<i>V</i><sub>p</sub>, which is comparable to a typical microwave antenna at the same microwave power, making SCHBAR a power-efficient device useful for fast spin control, dressed state coherence protection, and quantum circuit integration.