Laser pulses with Quantum-Random Polarisation

MetadataDetails
Publication Date2020-01-01
AuthorsDouglas J. Little, Ondřej Kitzler, Alexei Gilchrist, Richard P. Mildren
InstitutionsMacquarie University

We report the generation of Raman laser pulses in diamond with quantum-random polarisation, whereby laser pulses exhibit a coherent, well-defined, linear polarisation with an orientation that is random from pulse to pulse. Ā© 2020 The Author(s)