Skip to content

Synthetic diamond lenses for multi-spectral imaging

MetadataDetails
Publication Date2020-03-03
AuthorsFrederick Faulkner, Andrew M. R. Bennett, Daniel J. Twitchen
InstitutionsElement Six (United Kingdom)
Citations1

Traditionally the extreme hardness of diamond materials has made the machining of diamond optical components exceptionally difficult and limited applications to mostly flat components. Recent advances in diamond processing technology have made it possible to fabricate curved optical components or lenses in single crystal and polycrystalline diamond. This paper analyses a multi-spectral infrared imaging system incorporating a diamond lens and compares performance to equivalent systems that use other common infrared optical materials. Due to the broad transmission spectrum of diamond, which ranges all the way from the UV to microwave, these curved optics could find use in many different imaging applications throughout the electro-magnetic spectrum. Consideration is given to other advantages that diamond brings to the multi-spectral imaging application including small variations in refractive index as a function of both wavelength and temperature, a large Abbe number and material resilience under harsh conditions. As the development of large-area single crystal (SC) chemical vapour deposition (CVD) diamond advances, SC diamond lenses for multispectral imaging become a real possibility, with a number of advantages that we present in this paper.

  1. 2013 - CVD diamond for high power laser applications
  2. 2016 - Spectroscopy: CVD diamond attenuated-total-reflection prisms benefit FTIR spectroscopy
  3. 2015 - Diamond optical components for high-power and high-energy laser applications
  4. 2012 - Common aperture multispectral optics for military applications
  5. 1997 - Spectral imaging applications: remote sensing, environmental monitoring, medicine, military operations, factory automation, and manufacturing