Gigabit per second visible light communication based on AlGaInP red micro-LED micro-transfer printed onto diamond and glass
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-04-03 |
| Journal | Optics Express |
| Authors | J. F. C. Carreira, Enyuan Xie, Rui Bian, Johannes Herrnsdorf, Harald Haas |
| Citations | 25 |
Abstract
Section titled āAbstractāFull-color smart displays, which act both as a display and as a high-speed visible light communication (VLC) transmitter, can be realized by the integration of red-green-blue micron-sized light emitting diodes (micro-LEDs) onto a common platform. In this work, we report on the integration of aluminum gallium indium phosphide red micro-LEDs onto diamond and glass substrates by micro-transfer printing and their application in VLC. The device on-diamond exhibits high current density and bandwidth operation, enabled by diamondās superior thermal properties. Employing an orthogonal frequency division multiplexing modulation scheme, error-free data rates of 2.6 Gbps and 5 Gbps are demonstrated for a single micro-LED printed on-glass and on-diamond, respectively. In a parallel configuration, a 2x1 micro-LED array achieves error-free data rates of 3 Gbps and 6.6 Gbps, on-glass and on-diamond, respectively.