Anomalous Behavior of 2D Janus Excitonic Layers under Extreme Pressures
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2020-07-06 |
| Journal | Advanced Materials |
| Authors | Han Li, Ying Qin, Byeongkwan Ko, Dipesh Trivedi, Debarati Hajra |
| Institutions | Arizona State University |
| Citations | 63 |
Abstract
Section titled âAbstractâAbstract Newly discovered 2D Janus transition metal dichalcogenides layers have gained much attention from a theory perspective owing to their unique atomic structure and exotic materials properties, but little to no experimental data are available on these materials. Here, experimental and theoretical studies establish the vibrational and optical behavior of 2D Janus S-W-Se and S-Mo-Se monolayers under high pressures for the first time. Chemical vapor deposition (CVD)âgrown classical transition metal dichalcogenides (TMD) monolayers are first transferred onto van der Waals (vdW) mica substrates and converted to 2D Janus sheets by surface plasma technique, and then integrated into a 500 ”m size diamond anvil cell for highâpressure studies. The results show that 2D Janus layers do not undergo phase transition up to 15 GPa, and in this pressure regime, their vibrational modes exhibit a nonmonotonic response to the applied pressures ( dÏ / dP ). Interestingly, these 2D Janus monolayers exhibit unique blueshift in photoluminescence (PL) upon compression, which is in contrast to many other traditional semiconductor materials. Overall theoretical simulations offer inâdepth insights and reveal that the overall optical response is a result of competition between the ab âplane (blueshift) and c âaxis (redshift) compression. The overall findings shed the very first light on how 2D Janus monolayers respond under extreme pressures and expand the fundamental understanding of these materials.