Coherent Manipulation with Resonant Excitation and Single Emitter Creation of Nitrogen Vacancy Centers in 4H Silicon Carbide

MetadataDetails
Publication Date2020-07-09
JournalNano Letters
AuthorsZhao Mu, S. A. Zargaleh, H. J. von Bardeleben, Johannes E. Fröch, Milad Nonahal
InstitutionsUniversity of Technology Sydney, Nanyang Technological University
Citations75

Silicon carbide (SiC) has become a key player in the realization of scalable quantum technologies due to its ability to host optically addressable spin qubits and wafer-size samples. Here, we have demonstrated optically detected magnetic resonance (ODMR) with resonant excitation and clearly identified the ground state energy levels of the NV centers in 4H-SiC. Coherent manipulation of NV centers in SiC has been achieved with Rabi and Ramsey oscillations. Finally, we show the successful generation and characterization of single nitrogen vacancy (NV) center in SiC employing ion implantation. Our results highligh the key role of NV centers in SiC as a potential candidate for quantum information processing.