Formation of Multilayered Nanostructures of NV Sites in Single-Crystal CVD Diamond

MetadataDetails
Publication Date2020-07-01
JournalTechnical Physics Letters
AuthorsА. М. Горбачев, M. A. Lobaev, D. B. Radishchev, A. L. Vikharev, С. А. Богданов
InstitutionsInstitute for Physics of Microstructures, Institute of Applied Physics
Citations1

The results of growing multilayered nitrogen-doped nanostructures that have the form of periodically arranged nanometer-thick nitrogen-containing layers in a single-crystal CVD diamond are presented. The possibility of creating nitrogen-doped diamond layers with extremely sharp boundaries (less than 1 nm) is demonstrated. The photoluminescence study have shown that multilayered structures make it possible to obtain a higher radiation intensity of practically important NV - sites at a spin coherence time close to that for uniformly doped layers with the same concentration of nitrogen.