Skip to content

Microstructure and Properties of Nickel/Detonated Nanodiamond Composites Fabricated by Powder Metallurgy

MetadataDetails
Publication Date2020-07-08
JournalMaterials Performance and Characterization
AuthorsEman Toulba, Mahmudun Nabi Chowdhury, Ahmed I. Ali, Ibrahim S. Qassem, Walid M. Daoush
InstitutionsIslamic University, British University in Egypt
Citations1

ABSTRACT Nickel/detonated nanodiamond composites were prepared using the powder metallurgy technique. Detonated nanosized diamond particles were reinforced in the nickel matrix. The investigated powder was used to prepare homogenous diamond/nickel composite mixtures with different detonated nanodiamond content of weight percentage (0.2, 0.4, 0.6, and 0.8 wt.%). The produced mixtures were cold pressed into a cylindrical die shape under compaction pressure of 400 MPa followed by sintering at 1,000°C for 120 min under a controlled atmosphere of 1:3 hydrogen/nitrogen gas mixture. Phase identification and microstructure of the produced sintered samples were investigated using X-ray diffraction and scanning electron microscope, respectively. The results of the microstructure show a good distribution of the detonated nanodiamond in the nickel matrix, especially in the 0.8 wt% diamond/nickel sintered sample. The densities of the obtained sintered samples were measured by applying the Archimedes principal. As the detonated nanodiamond content was increased in the nickel matrix, the density of the sintered samples was decreased. The thermal expansion, electrical conductivity, and hardness of the produced diamond/nickel composites were measured. The coefficient of thermal expansion and electrical conductivity were decreased, but the hardness was increased by increasing the detonated nanodiamond weight percentage.

  1. 2004 - On the History of the Discovery of Nanodiamond Synthesis [Crossref]
  2. 2012 - The Properties and Applications of Nanodiamonds [Crossref]
  3. 2008 - Diamond Nanoparticles: Jewels for Chemistry and Physics [Crossref]
  4. 2009 - Nano Diamond Particles: Properties and Perspectives for Bioapplications [Crossref]
  5. 2007 - Sintering of Polycrystalline Diamond Cutting Tools [Crossref]
  6. 1961 - Formation of Diamond by Explosive Shock [Crossref]
  7. 2002 - Interaction of Neutrons with Nanoparticles [Crossref]
  8. 2017 - Advanced Diamond-Reinforced Metal Matrix Composites via Cold Spray: Properties and Deposition Mechanism [Crossref]
  9. 2012 - Effect of Combined Addition of Cu and Aluminum Oxide Nanoparticles on Mechanical Properties and Microstructure of Al-7Si-0.3Ā Mg Alloy [Crossref]
  10. 2015 - Synthesis of Micro- and Nanoparticles of Metal Oxides and Their Application for Reinforcement of Al-Based Alloys [Crossref]