Full thermal characterization of AlGaN/GaN high electron mobility transistors on silicon, silicon carbide, and diamond substrates using a reverse modeling approach
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2020-11-09 |
| Journal | Semiconductor Science and Technology |
| Authors | Assaad El Helou, Yue Cui, Marko J. Tadjer, Travis J. Anderson, Daniel Francis |
| Institutions | United States Naval Research Laboratory, Southern Methodist University |
| Citations | 12 |
Abstract
Section titled āAbstractāAbstract Gallium nitride (GaN) high electron mobility transistors (HEMTs) operate at high power levels and are thus especially thermally-critical devices. Not only do they require innovative thermal management strategies, but can also benefit from advanced experimental thermal characterization, both numerical and experimental, in their design and system integration stages. The thermal numerical analysis of microelectronic devices faces the challenges of complex physics and uncertain thermophysical properties which leads to numerically expensive models that are prone to error. By the use of an innovative reverse modeling approach to mitigate the above challenges, this work presents the full thermal characterization of GaN power devices with different substrates aimed at managing performance-limiting self-heating. The approach develops and optimizes a thermal simulation model to match the numerical results to experimentally-obtained thermal maps of the devices under test. The experimentally-optimized simulation model can then be used to extract full 3D temperature distributions, infer in-situ thermal properties, and provide a numerical platform that can be used to conduct further parametric studies and design iterations. The presented analysis provides a full thermal characterization of different GaN HEMT devices and compares the thermal performance of different substrates on the basis of thermal properties. The extracted properties for HEMTs on Si, SiC, and Diamond substrates are compared and a set of conclusions are presented to guide further developments in GaN HEMT thermal management strategies.
Tech Support
Section titled āTech SupportāOriginal Source
Section titled āOriginal SourceāReferences
Section titled āReferencesā- 2010 - GaN power switching devices [Crossref]