Zinc‐Ion Supercapacitors - Flexible Diamond Fibers for High‐Energy‐Density Zinc‐Ion Supercapacitors (Adv. Energy Mater. 44/2020)
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2020-11-01 |
| Journal | Advanced Energy Materials |
| Authors | Ze Jian, Nianjun Yang, Michael Vogel, Stewart Leith, Anna Schulte |
| Institutions | University of Siegen, City University of Hong Kong |
Abstract
Section titled “Abstract”In article number 2002202, Nianjun Yang, Xin Jiang and co-workers employ diamond fibers with a fibrous core/shell structure to assemble zinc-ion supercapacitors, which exhibit high gravimetric and volumetric energy and power densities, along with long-term stability and high flexibility. These diamond zinc-ion supercapacitors have promise as energy suppliers for flexible and wearable electronics.