Stimulated Raman scattering in suspension of submicron diamond particles

MetadataDetails
Publication Date2020-12-01
JournalJournal of Physics Conference Series
AuthorsA. N. Baranov, Dongxue Bi, В. С. Горелик, A. D. Kudryavtseva, A.N. Maresev
InstitutionsLomonosov Moscow State University, P.N. Lebedev Physical Institute of the Russian Academy of Sciences
AnalysisFull AI Review Included
  • Core Discovery: First experimental observation of Stimulated Raman Scattering (SRS) in a liquid suspension of submicron diamond particles, expanding the matrix of Raman-active media beyond bulk crystals.
  • Material Source: Particles synthesized via High Pressure High Temperature (HPHT) methods, exhibiting a characteristic Raman frequency shift of 1332 cm-1, corresponding to the fundamental optical F2g mode.
  • Optical Phenomena Detected: Simultaneous generation of Stokes and anti-Stokes SRS components, stimulated low-frequency Raman scattering, and multiphoton excited luminescence from negatively-charged nitrogen-vacancy (NV-) centers.
  • Application Target: Validates submicron diamond as an efficient, low-threshold active medium for compact Raman converters, quantum light sources, and biomedical imaging.
  • Key Advantage: Suspension-based format enables novel optofluidic device geometries impossible with rigid bulk diamond crystals.
  • Current Industry Need: A scalable supply of high-purity, narrow-size-distribution submicron diamond particles with reproducible optical quality for systematic nonlinear optics research.
  • Gap Addressed: Bridges the fields of diamond crystallography and colloid optics, creating a new platform for studying size-dependent quantum phenomena in diamond.
ParameterValueUnitContext
Raman frequency shift1332cm-1Fundamental F2g optical phonon mode of diamond
Diamond typeHPHT (High Pressure High Temperature) synthesized—Submicron particle form
Suspension mediumEthanol—Liquid carrier for SRS experiments
Particle size (hydrodynamic radius)<100nmSubmicron regime
Wavelength transparency range230 - 2500nmBroad optical window for diamond
SRS gain regimeStimulated—Both Stokes and anti-Stokes components observed
NV- center emissionZPL ~637nmNegatively-charged nitrogen-vacancy luminescence
Anti-Stokes generationConfirmed—High-order components via four-wave mixing
Thermal conductivityHighest of known materialsW/(m·K)Property enabling high-power SRS
Thermal expansion coefficientLow10-6/°CContributes to optical damage resistance
  • Particle Synthesis: Production of submicron diamond particles using High Pressure High Temperature (HPHT) methods, yielding crystallites with the characteristic 1332 cm-1 Raman signature.
  • Suspension Preparation: Dispersion of HPHT diamond particles in ethanol to create a stable liquid-phase optical medium suitable for nonlinear light-matter interaction studies.
  • Excitation Source: Pulsed laser pumping (referenced Nd3+:Y3Al5O12 laser systems used in comparable diamond SRS studies) delivered at energies above the SRS threshold.
  • Spectral Detection: Recording of Stokes and anti-Stokes frequency components via spectrometric analysis to confirm the 1332 cm-1 shift and identify higher-order phonon processes.
  • Low-Frequency Raman Mapping: Detection of stimulated low-frequency modes indicating acoustic phonon contributions within the suspended particles.
  • NV- Luminescence Characterization: Multiphoton pumping of NV centers to record Zero-Phonon Line (ZPL) emission and phonon sidebands, confirming nitrogen vacancy incorporation.
  • Threshold Measurement: Energy threshold determination for the onset of SRS in the suspension to compare with bulk diamond reference data.
  • Applicable Materials:

    • For replication and extension of this HPHT submicron diamond suspension work, 6CCVD recommends its Optical Grade Single Crystal Diamond (SCD) and Polycrystalline Diamond (PCD) feedstock. Our CVD-grown diamond offers a controlled nitrogen vacancy profile suitable for NV- photoluminescence and quantum emission studies.
    • For particle/slurry applications, bulk PCD plates or wafers can be precisely milled to provide high-purity, well-characterized diamond source material with reproducible Raman signatures at 1332 cm-1.
    • For quantum-grade NV center applications requiring enhanced nitrogen incorporation, our Boron-Doped Diamond (BDD) and selectively-engineered SCD products can be evaluated for tailored NV density.
  • Customization Potential:

    • Particle Size Engineering: Starting from bulk PCD or SCD substrates (available up to 125mm diameter and thicknesses from 0.1µm to 500µm), custom particle size fractions can be specified for your suspension protocol.
    • Metalization for Hybrid Optofluidic Devices: When transitioning from suspension experiments to integrated waveguide or microfluidic platforms, 6CCVD provides in-house metalization with Au, Pt, Pd, Ti, W, and Cu. A Ti/Pt/Au stack is ideal for gold-bonded hybrid integration with laser diode pump modules.
    • Laser Cutting & Shaping: Substrates can be laser-cut to user-defined geometries, enabling custom cuvette windows or waveguide end-facets compatible with your SRS experimental cell.
    • Surface Polishing: Our SCD polishing achieves Ra < 1nm, critical for minimizing scattering losses in any bulk diamond reference cell used alongside suspension measurements.
  • Engineering Support:

    • The authors’ work demonstrates that both the Raman gain at 1332 cm-1 and NV- photoluminescence can be simultaneously exploited. 6CCVD’s in-house PhD engineering team can advise on material selection between SCD, PCD, and BDD to optimize either the Raman conversion efficiency or the NV- luminescence yield for your specific experimental setup.
    • For researchers considering scaling this work from suspension to waveguide-integrated diamond photonics, our team can guide the transition from particulate systems to polished thin-film CVD diamond membranes.
  • Call to Action:

    • For custom specifications, material consultation, or bulk CVD diamond supply for nonlinear optics and quantum photonics research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract

Abstract We report on the first experimental observation of stimulated Raman scattering (SRS), stimulated low-frequency Raman scattering and multiphoton excited negatively-charged single nitrogen-vacancy (NV-) centers luminescence in ethanol suspension of submicron diamond particles obtained at high pressures and temperatures (HPHT). The Stokes and anti-Stokes SRS components with a frequency shift of 1332 cm −1 , corresponding to the fundamental optical mode of diamond crystal were observed. The spectral characteristics and energy thresholds of the studied processes were determined.