Dipole-Dipole Interactions Between Pairs of Silicon-Vacancy Centers in Diamond

MetadataDetails
Publication Date2021-01-01
JournalConference on Lasers and Electro-Optics
AuthorsMatthew W. Day, Kelsey M. Bates, Christopher L. Smallwood, Rachel Owen, Ronald Ulbricht
InstitutionsSan Jose State University, University of Michigan
Citations1

Silicon-vacancy centers in diamond are leading candidates for future quantum telecommunications, memory, and computing applications. We report dipole-dipole interactions between distinct silicon-vacancy centers in diamond with implications for quantum sensing and information exchange between centers.