Efficient linewidth compression to the Fourier limit via resonant phonon interaction in diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Authors | E. Granados, C. Granados, Rizwan Ahmed, K. Chrysalidis, V. N. Fedosseev |
| Institutions | Macquarie University |
Abstract
Section titled āAbstractāWe report on large power spectral density enhancement (~40 Ć ) of high power nanosecond lasers via coherent Raman conversion in an Fabry-PĆ©rot diamond resonator. The device produced directly a phase locked, near Fourier-limited Stokes output without the need of cavity length stabilization.