A Vertically Loaded Diamond Microdisk Resonator (VLDMoRt) towards a Scalable Quantum Network
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2021-01-01 |
| Journal | Conference on Lasers and Electro-Optics |
| Authors | Yuqin Duan, Kevin C. Chen, Dirk Englund, Matthew E. Trusheim |
| Institutions | Cambridge Electronics (United States) |
Abstract
Section titled āAbstractāWe design and fabricate a vertically loaded diamond microdisk resonator (VLDMoRt) that enhances spin-photon entanglement generation and free-space fiber- matched coupling rate from quantum emitters.