Electroluminescence of porous silicon carbide is achieved in a forward-biased SiC p-i-n junction. A broad green spectral feature centered at ∼510 nm is shown to arise from porous SiC. A large SiC surface area in the vicinity of the junction is created by diamond cutting followed by an electrochemically enhanced hydrogen fluoride etch that produces a layer of porous SiC. Photoluminescence is shown not to be responsible for the green emission. This supports the model of carrier recombination at the porous region via lateral bipolar diffusion of carriers. A lateral bipolar diffusion model is presented in which mobile carriers diffuse laterally from the junction toward the porous SiC surface region driven by a lateral carrier concentration gradient. Lateral bipolar diffusion in conjunction with suitable radiative recombination centers provides a possible pathway to achieve high quantum efficiencies in future SiC p-n homojunction or double heterojunction light-emitting diodes. Competing recombination processes and associated ideality factors in 4H-SiC diodes are also examined.

  1. 2014 - Fundamentals of Silicon Carbide Technology, Growth, Characterization, Devices, and Applications
  2. 2013 - Silicon carbide light emitting diode as a prospective room temperature source for single photons [Crossref]
  3. 1998 - Photoluminescence and transport studies of boron in 4H SiC [Crossref]
  4. 1994 - Emission of blue light from hydrogenated amorphous silicon carbide [Crossref]
  5. 2017 - Effective optimization of surface passivation on porous silicon carbide using atomic layer deposited Al2O3 [Crossref]