Executive Summary
Section titled “Executive Summary”- Application: Single-Crystal Chemical Vapour Deposition (scCVD) diamond pixelated detector utilizing buried graphitic electrodes (XBPM) for synchrotron beam diagnostics.
- Core Innovation: All-carbon, transmissive X-ray beam position monitor (XBPM) featuring internal graphitic wire electrodes fabricated via pulsed-laser writing, eliminating standard surface metallization.
- Key Performance: Achieved sub-micron beam position accuracy and 100 FPS imaging in 4th generation synchrotron beamlines with linear intensity response across three orders of magnitude.
- Detector Material: High-purity, optical-grade scCVD diamond plate (50 µm thickness) offering superior X-ray transmissivity (>4 keV photons) compared to Si, SiC, Ge, and LuAG/YAG scintillators.
- Operational Endurance: Intrinsically radiation-tolerant design; buried electrodes are immune to surface damage from high-flux X-ray beams.
- Target Use Cases: Sub-micron X-ray beam profiling, adaptive optics feedback loops, particle tracking at colliders, and synchrotron fault-finding diagnostics.
- Related Numerical Work: Diffusion-based carrier motion modeling is applied to evaluate the spatial charge collection efficiency of various 3D wire/pillar geometries.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Detector Material | scCVD Diamond | — | High-purity, radiation-tolerant transmissive aperture |
| Plate Thickness | 50 | µm | Optimized for minimum absorption of >4 keV X-rays |
| Active Aperture Dimensions | ~2100 x 2100 | µm² | Total measured mapped area |
| Electrode Geometry | HT X & HT Y Wire Patterns | — | Orthogonal buried graphitic electrodes |
| Wire Spacing (Pitch) | 100 / 250 | µm | Defines pixel resolution nodes |
| Electrode Fabrication | Pulsed-Laser Writing | — | Creates buried conductive graphitic tracks |
| Contact Pads (Surface) | Ti / Au | — | Pad metallization only (external wire bonds) |
| Imaging Rate | 100 | FPS | Read out via modulation lock-in technique |
| Beam Position Resolution | sub-micron | µm | Goal achieved under operational conditions |
| Dynamic Range (Intensity) | 3 | Orders of Magnitude | Validated linear response with downstream flux monitors |
| Photon Energy Range | 4 - 100 | keV | Operational transmission window |
| Incident Photon Flux (Synchrotron) | up to 1x10¹⁴ | photons/s | High-flux synchrotron beamline environment |
| Beam Stability Goal | < 10% of beam size / <1% beam intensity | — | 3rd generation synchrotron metrics |
Key Methodologies
Section titled “Key Methodologies”- Material Selection: Utilize high-purity Single Crystal CVD (scCVD) diamond, exploiting its wide bandgap (~5.5 eV), radiation hardness, and low atomic number for minimal beam perturbation.
- Preparation: Polish the scCVD diamond plate down to the 50 µm target thickness. Optical-grade surface finishing is essential to avoid scattering artifacts.
- Electrode Fabrication: Use a pulsed-laser technique to write subsurface graphitic wires directly inside the diamond plate. The graphitization forms continuous conductive tracks beneath a thin diamond surface layer.
- Metallization: Deposit Ti/Au contact pads solely for external wire-bonded interfaces, keeping the central transmissive aperture completely metallization-free.
- Device Integration: Mount the diamond sensor into a motorized chamber. Install immediately downstream of beamline defining slits.
- Readout Architecture: Drive electrodes with modulated bias supplies (e.g., 1 kHz to 25 kHz frequencies). Use lock-in amplifiers synchronized to the modulation frequencies.
- Signal Processing: Employ a lock-in algorithm to simultaneously read every pixel. Calculate beam centroid and intensity via Fourier transform amplitude summation.
- Performance Validation: Scan the detector across the beam in 10 µm steps. Use a downstream ion chamber as the independent intensity reference to confirm linearity.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”This research highlights advanced demands in synchrotron instrumentation and high-energy physics: specifically, the need for flawless diamond bulk material supporting novel 3D buried-electrode geometries. 6CCVD provides the foundational technology required to fabricate and scale such devices.
Applicable Materials:
- Optical Grade SCD: The investigators utilized high-purity, double-side polished scCVD diamond. Our electronic-grade single crystal diamond is grown via MPCVD and manufactured to specifications supporting demanding X-ray transmission and charge transport applications.
- Custom Geometry Free-Standing SCD: To produce the paper’s 50 µm transmissive plate, raw crystalline material must be precision-thinned and polished. 6CCVD provides SCD plates spanning 0.1 µm - 500 µm, with sub-nanometer surface roughness (Ra < 1 nm), ensuring maximum photon transmission without unnecessary absorption or scattering.
- Intrinsic PCD (Detector Grade): For applications requiring higher volume manufacturing costs or larger active areas, our polycrystalline MPCVD diamond provides a robust alternative while retaining radiation hardness.
Customization Potential:
- Precision Thinning & Sizing: Achieving the paper’s exact 50 µm active membrane requires specialized handling. We provide laser cutting and precision lapping/polishing to achieve exact thickness requirements without compromising structural integrity.
- Custom Metalization: The paper describes Ti/Au contact pads. 6CCVD offers internal, in-house metalization capabilities using Au, Pt, Pd, Ti, and W. We can engineer multilayer contact pad stacks and patterned traces designed specifically to mate with your embedded graphitic wires.
- Wafer Scale Manufacturing: For extension to larger XFEL or collider beamline monitors (e.g., 100mm or 125mm formats), our PCD capabilities provide scalable active areas. We supply free-standing PCD substrates up to 10mm thick.
Engineering Support:
- Implementing novel 3D graphitic electrodes requires deep knowledge of crystal defects, laser-matter interaction thresholds, and charge carrier dynamics in diamond. Our in-house PhD engineering team assists clients in material selection, boundary condition simulations, and prototyping complex detector geometries.
- We provide consultation on optimal crystal orientations for laser-written conducting tracks and evaluate substrate strategies to maximize Charge Collection Efficiency (CCE) for your exact energy range and experimental apparatus.
Call to Action: For custom diamond detector specifications or material consultation to advance your synchrotron, XFEL, or particle tracking research, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
A new type of transmissive pixel detector has been developed for synchrotron radiation diagnostics at Diamond Light Source. A thin single-crystal CVD diamond plate is used as the detector material, and a pulsed-laser technique has been used to write conductive graphitic electrodes inside the diamond plate. Instead of using traditional electrodes formed from a layer of surface metallisation, the graphitic electrodes are buried under the surface of the diamond and result in an all-carbon imaging detector. Within the instrument’s transmissive aperture there are no surface structures that could be damaged by exposure to radiation beams, and no surface metallization that could introduce unwanted absorption edges. The instrument has successfully been used to image the X-ray beam profile and measure the beam position to sub-micron accuracy at 100 Hz at Diamond Light Source. A novel modulation lock-in technique is used to read out all pixels simultaneously. Presented in this work are measurements of the detector’s beam position resolution and intensity resolution. Initial measurements of the instrument’s spread-function are also presented. Numerical simulations are used to identify potential improvements to the electrode geometry to improve the spatial resolution of similar future detectors. The instrument has applications in both synchrotron radiation instrumentation, where real-time monitoring of the beam profile is useful for beam diagnostics and fault-finding, and particle tracking at colliders, where the electrode geometries that buried graphitic tracks can provide increased the charge collection efficiency of the detector.