Characterization of pavement surface undulations using side view images

MetadataDetails
Publication Date2021-02-01
JournalIOP Conference Series Materials Science and Engineering
AuthorsSubham Jain, Animesh Das
InstitutionsIndian Institute of Technology Kanpur
Citations1

Abstract Pavement surface undulations affect friction, ride comfort, water drainage, noise etc. Various indices have been proposed in the literature to characterize the pavement surface undulations. The present paper compares a few pavement surface undulation indices in the spatial domain and the frequency domain. For this study, core samples of pavement surface were collected from freshly constructed pavements, which had not been opened to the traffic yet. The core samples were sliced using a high-speed diamond saw. Images of the side view of the slices were captured using a digital camera. Suitable image processing scheme was employed to detect the pavement surface profiles. Various indices were subsequently estimated and compared.

  1. 2004 - Drainage considerations for porous asphalt surface course design [Crossref]
  2. 1996 - Characterization of pavement surface texture and its influence on tire/road noise
  3. 2012 - Laser scanning on road pavements: a new approach for characterizing surface texture [Crossref]
  4. 2010 - Laser-triangulation device for in-line measurement of road texture at medium and high speed [Crossref]
  5. 2011 - Toward low-cost 3D automatic pavement distress surveying: the close range photogrammetry approach