Distribution of Clusters Formed by sp2- and sp3-Bonds in a Carbon Diamond-like Thin Film
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2021-05-01 |
| Journal | Technical Physics |
| Authors | В. А. Плотников, С. В. Макаров, O. O. Eremeenkova, A. A. Shutkin |
| Institutions | Altai State University |
Abstract
Section titled “Abstract”Experimental studies of carbon thin films obtained by condensation of carbon from the vapor-gas phase onto a metal substrate are presented. Evaporation of graphite targets is carried out by defocused laser radiation. Using transmission electron microscopy, scanning probe microscopy, and Raman spectra, it is shown that the structure of the carbon film consists of large nonconducting diamond fragments with sp3-bonds, along the boundaries of which current regions with sp2-bonds are localized.