Recent developments of quantum sensing under pressurized environment using the nitrogen vacancy (NV) center in diamond

MetadataDetails
Publication Date2021-06-24
JournalJournal of Applied Physics
AuthorsKin On Ho, King Cho Wong, Man Yin Leung, Yiu Yung Pang, Wai Kuen Leung
InstitutionsChinese University of Hong Kong, Chinese University of Hong Kong, Shenzhen
Citations26

Pressure has been established as a powerful way of tuning material properties and studying various exotic quantum phases. Nonetheless, measurements under pressure are no trivial matter. To ensure a stable pressure environment, several experimental restrictions must be imposed including the limited size of a sample chamber. These have created difficulties in assembling high-pressure devices and conducting measurements. Hence, novel sensing methods that are robust and compatible with high-pressure devices under pressure are highly in demand. In this review, we discuss the nitrogen-vacancy (NV) center in diamond as a versatile quantum sensor under pressure. The excellent sensitivity and superior resolution of the NV center enable exciting developments in recent years. The NV center has great potential in sensing under pressure, especially beneficial to magnetic-related measurements.

  1. 1996 - Metallization of fluid molecular hydrogen at 140 GPa (1.4 Mbar) [Crossref]
  2. 2020 - Synchrotron infrared spectroscopic evidence of the probable transition to metal hydrogen [Crossref]
  3. 2019 - Effects of hydrostatic pressure on the surface plasmon resonance of gold nanocrystals [Crossref]
  4. 2007 - On the glass temperature under extreme pressures [Crossref]
  5. 2019 - Evidence for superconductivity above 260 K in lanthanum superhydride at megabar pressures [Crossref]
  6. 2019 - Superconductivity at 250 K in lanthanum hydride under high pressures [Crossref]
  7. 2015 - Conventional superconductivity at 203 kelvin at high pressures in the sulfur hydride system [Crossref]
  8. 2020 - Room-temperature superconductivity in a carbonaceous sulfur hydride [Crossref]
  9. 2003 - Susceptibility measurements at high pressures using a microcoil system in an anvil cell [Crossref]