Comparison of back focal plane imaging of nitrogen vacancy centers in nanodiamond and core-shell CdSe/CdS quantum dots
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2022-01-01 |
| Journal | Journal of Physics Conference Series |
| Authors | Justus Christinck, Beatrice Rodiek, Marco López, Hristina Georgieva, Helmut Hofer |
| Institutions | Max Planck Institute for the Science of Light, Physikalisch-Technische Bundesanstalt |
| Citations | 1 |
| Analysis | Full AI Review Included |
Back Focal Plane Imaging of NV Centers & Quantum Dots: Technical Documentation
Section titled “Back Focal Plane Imaging of NV Centers & Quantum Dots: Technical Documentation”- Objective: Characterize angular-dependent emission of two single-photon emitters (NV-center in nanodiamond vs. core-shell CdSe/CdS quantum dots).
- Methodology: Confocal microscopy combined with back focal plane (BFP) imaging and Hanbury-Brown and Twiss (HBT) interferometry.
- Key Finding: The Lukosz-Kunz theoretical model accurately predicts 2D dipole emission patterns for both emitter types.
- NV-Center Orientation: θ = 60° ± 4°, φ = 334° ± 2°.
- QD Orientation: θ = 30° ± 4°, φ = 35° ± 2°.
- NV Emission Band: 600 nm - 750 nm (broad spectrum).
- QD Emission Band: Centered at ~640 nm, FWHM = 20 - 40 nm.
- Metrology Target: Achieve photon rates > 330,000 photons/s for absolute calibration of Si-SPAD detectors.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Excitation Wavelength | 532 | nm | CW laser source |
| Objective NA (NV-center) | 1.45 | - | Oil-immersion |
| Objective NA (QD) | 1.4 | - | Oil-immersion |
| Spectral Filter Cutoff | 550 - 750 | nm | Bandpass range |
| Bertrand Lens Focal Length | 500 | mm | Back focal plane imaging |
| Detector Type | Si-SPAD | - | HBT interferometer |
| Camera | sCMOS | - | Angular emission recording |
| Nanodiamond Diameter | ~75 | nm | 0.15 GAF grade, Microdiamond AG |
| QD Diameter (CdSe/CdS) | ~15 | nm | Core-shell architecture |
| NV-Center Emission Range | 600 - 750 | nm | ZPL + phonon sideband |
| QD Emission Peak | ~640 | nm | Narrow-band emission |
| QD Emission FWHM | 20 - 40 | nm | Spectral bandwidth |
| NV g(2)(0) Target | < 0.5 | - | Single-photon purity threshold |
| Irradiation Power Limit | > 50 | µW | Above this, QD bleaching observed |
| Refractive Index (Cover Glass) | ~1.52 | - | Dielectric interface medium |
| NV Orientation Angle θ | 60 ± 4 | ° | Out-of-plane dipole orientation |
| NV Orientation Angle φ | 334 ± 2 | ° | In-plane dipole orientation |
| QD Orientation Angle θ | 30 ± 4 | ° | Out-of-plane dipole orientation |
| QD Orientation Angle φ | 35 ± 2 | ° | In-plane dipole orientation |
Key Methodologies
Section titled “Key Methodologies”- Sample Preparation
- Nanodiamonds (0.15 GAF grade, ~75 nm) spin-coated onto standard cover glass.
- Core-shell CdSe/CdS quantum dots (~15 nm) drop-cast onto standard cover glass.
- Confocal Microscopy
- 532 nm CW excitation via neutral density filter and laser line filter.
- Dichroic beam splitter (DBS) separates excitation/emission paths.
- Single-mode fiber acts as confocal pinhole.
- Single-Photon Purity Verification
- Hanbury-Brown and Twiss (HBT) interferometer with two Si-SPADs.
- Second-order correlation function g(2)(τ) fitted with three-level model including timing jitter σ convolution.
- Back Focal Plane (BFP) Imaging
- Bertrand lens (500 mm focal length) inserted into detection path.
- Angular emission patterns recorded on sCMOS camera.
- Theoretical Modeling (Lukosz-Kunz)
- 2D dipole model at dielectric interface (cover glass / air).
- Equations differentiate s- and p-wave emission components.
- Orientation angles θ and φ extracted via least-squares fitting.
- Uncertainty Calculation
- 95% confidence bounds (Student’s t-distribution) for θ.
- Rectangular function algorithm utilizing BFP image symmetry for φ.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”This research requires high-purity, single-photon-grade diamond with precisely controlled NV-center formation. The following 6CCVD materials are directly applicable:
- Optical Grade Single Crystal Diamond (SCD) - Ideal for fabricating nanodiamonds or bulk substrates containing high-quality NV-centers with narrow inhomogeneous broadening.
- High-Pressure High-Temperature (HPHT) Grade SCD Substrates - Suitable as bulk platforms for NV-center studies where orientation-controlled emission (θ, φ) is critical.
- Boron-Doped Polycrystalline Diamond (BDD) - Available for researchers exploring charge-state stabilization of NV-centers via p-type doping.
Customization Potential
Section titled “Customization Potential”The paper’s angular emission analysis relies on emitters at a dielectric interface (cover glass / air, n ≈ 1.52). 6CCVD can support extension of this work:
- Custom Substrate Dimensions: Diamond plates/wafers up to 125 mm diameter (PCD) available for custom sample fabrication.
- Thickness Control: SCD and PCD films from 0.1 µm to 500 µm; bulk substrates up to 10 mm for advanced optical mounting.
- Surface Polishing:
- SCD: Ra < 1 nm - critical for minimizing optical scatter in BFP imaging.
- Inch-size PCD: Ra < 5 nm - suitable for hybrid nanophotonic device integration.
- Metallization Services: For advanced sample designs incorporating mirrors or antenna layers (as proposed in the paper’s conclusion), 6CCVD offers in-house deposition of Ti, Pt, Au, Pd, W, and Cu.
- Laser Cutting & Dicing: Nanodiamond arrays or patterned single-crystal membranes can be custom-cut to specified geometries.
Engineering Support
Section titled “Engineering Support”6CCVD’s in-house PhD engineering team specializes in:
- Material selection for quantum metrology and single-photon source development.
- Optimization of NV-center density via controlled nitrogen doping during MPCVD growth.
- Advising on dielectric interface engineering - e.g., diamond-on-MgF2 or diamond-on-PMMA heterostructures for enhanced photon collection efficiency, as suggested in the paper’s future-work section.
- Guidance on integrating diamond emitters with solid immersion lenses (SILs) or photonic antenna structures to exceed the 330,000 photons/s calibration threshold.
Application Relevance
Section titled “Application Relevance”| Research Requirement | 6CCVD Solution |
|---|---|
| Single NV-centers in nanodiamond | Optical-grade SCD nanodiamond feedstock |
| Bulk diamond for NV orientation studies | Custom-cut SCD substrates <1 nm Ra |
| Charge-state engineering | Boron-doped diamond (BDD) |
| Dielectric antenna layer integration | Metallization (Ti/Au, Pt) for mirror fabrication |
| Photon extraction enhancement | Ultra-polished SCD windows, laser-cut geometries |
For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Abstract We report on the characterization of the angular-dependent emission of two different single-photon emitters based on nitrogen-vacancy centers in nanodiamond and on core-shell CdSe/CdS quantum dot nanoparticles. The emitters were characterized in a confocal microscope setup by spectroscopy and Hanbury-Brown and Twiss interferometry. The angular-dependent emission is measured using a back focal plane imaging technique. A theoretical model of the angular emission patterns of the 2D dipoles of the emitters is developed to determine their orientation. Experiment and model agree well with each other.