Stretched three-dimensional white graphene with a tremendous lattice thermal conductivity increase rate

MetadataDetails
Publication Date2022-01-01
JournalRSC Advances
AuthorsYang Han, Yue Liang, Xiaochuang Liu, Shijie Jia, Chaoxiang Zhao
InstitutionsCentre d’ÉnergĂ©tique et de Thermique de Lyon, Centre National de la Recherche Scientifique
Citations4

Thermal conductivity of the 3D h-BN honeycomb structure increases by 7.2 times under strain compared to an increase of only 0.67 times in the strained 3D graphene counterpart, differing from behaviors of traditional bulk diamond or silicon.