Superfluorescence and Collective Purcell-Enhancement of Nitrogen Vacancy Centers in diamond membranes

MetadataDetails
Publication Date2022-01-01
JournalFrontiers in Optics + Laser Science 2022 (FIO, LS)
AuthorsMaximilian Pallmann, Kerim Kƶster, Julia Heupel, Cyril Popov, David Hunger
InstitutionsUniversity of Kassel, Karlsruhe Institute of Technology

We observe cavity-enhanced ensemble fluorescence of nitrogen-vacancy centers in diamond, showing Purcell-enhancement of the Zero Phonon Line (ZPL). The emission features temporal bunching of ZPL photons, indicating collective emission that can be attributed to superfluorescence.