In this study, the magnetic field-based abrasive grain patterning for the production of electroplating diamond wire saws was studied. During the manufacturing process of the electroplating diamond wire saw, a permanent magnet was used to perform magnetization of the carbon steel wire. In addition, the following two methods were further used to perform partial degaussing on the carbon steel wire. The first method refers to the laser degaussing method, and the second method refers to the electromagnetic degaussing method, followed by performing electroplating on the carbon steel wire that has undergone the degaussing process. The impacts of these two methods on the magnetization characteristics of the carbon steel wire were studied, the magnetic induction strength of the zone of degaussing, range of the zone of degaussing, production speed, etc., in order to reach a conclusion on the methods for degaussing of a carbon steel wire. In this study, a nanosecond laser with a wavelength of 355 nm was used to perform a partial degaussing treatment on the surface of a magnetized carbon steel wire. When the laser fluence is 11.56 J/cm2, the controlled degaussing region of the abrasive grains could be minimized to 83.8 μm.

  1. 2014 - Recovery of solar grade silicon from kerf loss slurry waste [Crossref]
  2. 2010 - Characterization of polycrystalline silicon wafers for solar cells sliced with novel fixed-abrasive wire [Crossref]
  3. 2013 - Multi-wire sawing of sapphire crystals with reciprocating motion of electroplated diamond wires [Crossref]
  4. 2016 - Phase and stress evolution in diamond microparticles during diamond-coated wire sawing of Si ingots [Crossref]
  5. 2000 - Photovoltaic materials, past, present, future [Crossref]
  6. 2018 - Diamond wire sawing of solar silicon wafers: A sustainable manufacturing alternative to loose abrasive slurry sawing [Crossref]
  7. 2003 - Development of a high-speed manufacturing method for electroplated diamond wire tools [Crossref]
  8. 2010 - The determination of parameters for ordered arrangement of diamonds in impregnated diamond bit [Crossref]
  9. 2014 - Distribution of diamond grains in fixed abrasive wire sawing process [Crossref]
  10. 2007 - Preparation of nanostructured Ni/Al2O3 composite coatings in high magnetic field [Crossref]