Observation of High-Order Laguerre-Gaussian Beams from a Diamond Raman Laser
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2022-07-31 |
| Authors | Hui Chen, Yu Zhang, Hongwei Guo, Jiashuo An, Zhenxu Bai |
| Institutions | Hebei University of Technology |
Abstract
Section titled āAbstractāWe report on the direct generation of LG <inf xmlns:mml=āhttp://www.w3.org/1998/Math/MathMLā xmlns:xlink=āhttp://www.w3.org/1999/xlinkā>0,m</inf> modes Stokes laser with m tunable range of 0-9, for the first time to our knowledge, in an external-cavity diamond Raman laser using Gaussian beam pumping.