Transitions in polycrystalline diamond probed by steady state, modulated and transient surface photovoltage spectroscopy
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2022-11-30 |
| Journal | Semiconductor Science and Technology |
| Authors | Thomas Dittrich, Steffen Fengler |
| Institutions | Helmholtz-Zentrum Berlin für Materialien und Energie, Helmholtz-Zentrum Hereon |
| Citations | 7 |
| Analysis | Full AI Review Included |
Transitions in Polycrystalline Diamond Probed by Surface Photovoltage Spectroscopy
Section titled “Transitions in Polycrystalline Diamond Probed by Surface Photovoltage Spectroscopy”Executive Summary
Section titled “Executive Summary”- Core Achievement: Highly sensitive Surface Photovoltage (SPV) spectroscopy across dc (Kelvin probe), ac (modulated), and ac (transient) regimes maps electronic transitions in polycrystalline CVD diamond spanning near-infrared to deep-ultraviolet (0.8-5.8 eV).
- Defect Fingerprint Catalog: Eight distinct defect transitions (D1-D8) were detected at 0.8-0.9, 1.0, 1.37, 1.78, 2.27, 3.15, 4.2, and 5.42 eV, providing a reference dataset for grain-boundary disorder, sp2 bonded carbon, and dangling bond states.
- Phonon-Assisted Bandgap Analysis: SPV resolved exciton-phonon replicas at Eg - Ex ± hνLA,LO (5.27 / 5.53 eV) and Eg - Ex + hνTO (5.60 eV) relative to diamond’s 5.47 eV indirect bandgap.
- Asymmetry Discovery: Nucleation-side vs. growth-side illumination revealed opposite charging polarity, with grain-boundary density driving preferential electron separation.
- Method Versatility: Demonstrated applicability to ultra-wide bandgap semiconductors beyond diamond (e.g., GaN, AlN, β-Ga2O3) for research and routine quality control.
- Noise Floor Benchmark: Achieved noise levels as low as < 0.5 µV (ac modulated) and ~ 30 µV (dc Kelvin) — establishing SPV as a viable non-destructive metrology tool for wide-bandgap materials.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Sample Type | Polycrystalline CVD diamond (Type II) | — | Window-grade, nucleation + growth sides characterized |
| Sample Thickness | 0.1 | mm | Commercial freestanding CVD window |
| Sample Area | 1 × 1 | cm2 | Standard substrate geometry |
| Hydrogen Content | < 1000 | ppm | Below detection of typical grain-boundary passivation |
| Silicon Content | Below detection limit | ppm | Nominally undoped |
| Nitrogen Content | Below detection limit | ppm | Nominally undoped |
| Indirect Bandgap (Eg) | 5.47 | eV | Reference [1] |
| Exciton Binding Energy (Ex) | 0.07 | eV | Reference [1] |
| LA/LO Phonon Energy (hνLA,LO) | 0.132 | eV | Reference [1] |
| D1 Transition Energy | 0.8-0.9 | eV | sp2 π → π∗ / dangling bond onset |
| D2 Transition Energy | 1.0 | eV | Dominant feature, π → π∗ at grain boundaries |
| D3 Transition Energy | 1.37 | eV | Broad energy distribution (multiple signatures) |
| D4 Transition Energy | 1.78-1.8 | eV | Bulk defect (substitutional nitrogen related) |
| D5 Transition Energy | 2.27 | eV | π → σ∗ in disordered phase |
| D6 Transition Energy | 3.15 | eV | π → σ∗ in disordered phase |
| D7 Transition Energy | 4.2-4.6 | eV | Valence to conduction band tails |
| D8 Transition Energy | 5.42 | eV | Near-bandgap defect, origin unclear |
| Phonon Replica 1 | 5.27 | eV | Eg - Ex - hνLA,LO |
| Phonon Replica 2 | 5.53 | eV | Eg - Ex + hνLA,LO |
| Phonon Replica 3 | 5.60 | eV | Eg - Ex + hνTO |
| Noise Floor (dc Kelvin) | ~ 30 | µV | Full spectrum < 30 min acquisition |
| Noise Floor (ac modulated) | ~ 3 | µV | Charge amplifier configuration |
| Noise Floor (high-Z buffer) | < 0.5 | µV | SnO2:F coated electrode + mica spacer |
| Noise Floor (transient, short time) | ~ 500 | µV | At 20 ns time gate |
| Noise Floor (transient, long time) | < 100 | µV | At times > 0.1 ms |
| Laser Repetition Rate | 0.25 | Hz | Transient SPV pulse rate |
| Averages per Data Point | 10 | — | Transient measurement |
Key Methodologies
Section titled “Key Methodologies”- Sample Selection: Polycrystalline CVD diamond window (0.1 mm thick, 1 × 1 cm2, Diamond Materials GmbH Type II, H < 1000 ppm).
- Three SPV Regimes on Identical Electrode / Position:
- dc (Kelvin probe) — Contact potential difference (CPD) measured with vibrating steel bar electrode.
- ac (modulated) — Lock-in amplifier with in-phase (X) and 90° phase-shifted (Y) detection.
- ac (transient) — Pulsed laser excitation (0.25 Hz), 10 averages, logarithmic time readout.
- Illumination Sources:
- Xe lamp for broadband UV-vis-NIR coverage.
- Halogen lamp for low-straylight NIR characterization.
- Tunable OPO / dye-laser system for photon-energy-resolved scans from ~ 0.5 to ~ 5.8 eV.
- Beam Conditioning: Motorized filter wheel for straylight suppression; beam expander with minimum zoom factor 2.5; cut-on filter (900 nm) for straylight-isolated measurements.
- Electrode Geometries:
- Perforated electrode + charge amplifier for dc/ac modulated regimes.
- SnO2:F coated electrode + mica spacer + high-impedance buffer (× 10 gain) for ultra-low-noise NIR measurements.
- Sample Orientation Protocol: Diamond flipped to compare nucleation-side vs. growth-side illumination under identical electrode positioning.
- Phonon-Assisted Transition Identification: Compared observed spectral features against literature values for indirect exciton-phonon coupling at 5.268, 5.531, and 5.615 eV.
- Derivative Spectroscopy: First-derivative of -ΔCPD spectra applied to enhance onset detection for closely spaced transitions.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials:
- The defect spectroscopy catalog in this work (D1-D8) requires CVD polycrystalline diamond with well-characterized nucleation and growth surfaces — 6CCVD Optical Grade PCD (polished to Ra < 5 nm on inch-size wafers) is ideally suited as a baseline substrate.
- For experiments probing the role of acceptor density near 1 eV, 6CCVD Heavy Boron-Doped PCD (BDD) enables controlled activation-energy tuning matching the dose-dependent shifts described in [21].
- For bandgap-edge phonon-assisted studies, 6CCVD High-Purity SCD (0.1-500 µm thickness) provides the crystalline baseline referenced in [30], where transient SPV signals were “up to about ten times larger” than on PCD.
-
Customization Potential:
- The 0.1 mm × 1 × 1 cm2 geometry used here is a standard reference, but SPV electrode contact geometry is application-specific. 6CCVD offers custom metalization (Ti / Pt / Au / Pd / W / Cu) and laser cutting to produce tailored electrode pad patterns and die dimensions without the need for customers to invest in post-processing metallization equipment.
- For straylight-sensitive NIR measurements, an SnO2:F transparent electrode is advantageous — 6CCVD can support TCO-compatible surface engineering on request.
-
Engineering Support:
- The paper demonstrates that measurement regime (dc vs. ac modulated vs. ac transient) dramatically alters observed sign and magnitude of defect-related SPV signals — a critical consideration for any group designing wide-bandgap semiconductor characterization workflows. 6CCVD’s in-house PhD team can assist with material selection for projects targeting photovoltaic, photocatalytic, bio-sensor, or power-electronics applications of polycrystalline and single-crystal diamond.
- 6CCVD substrates are available up to 125 mm diameter (PCD) and 10 mm thickness, with SCD / PCD / BDD variants covering the full parameter space required to extend this defect-state mapping from the bandgap into the device-relevant sub-bandgap regime.
-
Call to Action:
- For custom specifications, metalization stack design, or material consultation on wide-bandgap diamond characterization, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
Abstract Numerous electronic transitions in polycrystalline chemical vapor deposition diamond with characteristic nucleation and growth sides were obtained by highly sensitive surface photovoltage (SPV) spectroscopy in dc (Kelvin probe), ac (modulated) and ac (transient) regimes from near infrared to deep ultraviolet. In the dc regime, defect transitions D1 to D8 were detected at 0.8-0.9, 1, 1.37, 1.78, 2.27, 3.15, 4.2 and 5.42 eV, respectively. Hints for more transitions were found for measurements in the ac (modulated) regime in the range near D3. SPV measurements in the ac (transient) regime showed the importance of disorder for relaxation of SPV signals excited at different photon energies. Phonon assisted transitions were observed at E g − E x − hν LA,LO , E g − E x + hν LA,LO and E g − E x + hν TO . The developed SPV techniques are suitable for applications in research and quality control not only for diamond but also for any other semiconductor with ultra-wide bandgap.