Skip to content

Submicrometer-scale temperature sensing using quantum coherence of a superconducting qubit

MetadataDetails
Publication Date2023-01-01
JournalNew Journal of Physics
AuthorsKosuke Kakuyanagi, Hiraku Toida, L. V. Abdurakhimov, Shiro Saito
InstitutionsNTT Basic Research Laboratories
Citations6
AnalysisFull AI Review Included

Submicrometer-Scale Quantum Thermometry via Superconducting Qubit-Diamond Hybrid Systems

Section titled “Submicrometer-Scale Quantum Thermometry via Superconducting Qubit-Diamond Hybrid Systems”
  • Pioneering Sensitivity: Achieved ultra-high temperature sensitivity of 1.3 µK / √Hz at T = 9.1 mK using quantum coherence of a superconducting flux qubit coupled to nano-diamonds.
  • Spatial Resolution Breakthrough: Submicrometer-scale thermometry enabled by detecting magnetization of 140 nm HPHT-grown nano-diamonds distributed directly on qubit structures.
  • Novel Sensing Architecture: Polarization of P1 center electron spins (S = 1/2) in diamond converts temperature shifts into magnetic field signatures, readable via Ramsey interference.
  • Wide Dynamic Range: Linear response from 50 mK down to 20 mK with slope dB⊥,M / dT⁻¹ = 6.158 nT·K; self-calibrating below resistance thermometer accuracy thresholds.
  • Minimal Thermal Footprint: Nano-diamond heat capacity is negligible compared to substrate, preserving the target temperature during measurement.
  • Quantum-Enhanced Performance: Sensitivity scales with magnetic field strength (B∥), with predicted 2.4× improvement at optimal B∥^opt = 10.1 mT.
  • Robust Stability: Allan deviation analysis confirms dominant white noise up to 100 ms, with 1/f noise taking over around 1 second for reliable long-term integration.
ParameterValueUnitContext
Energy gap of qubit (Δ/h)5.16GHzQubit characterization at base temperature
Persistent loop current (Iₚ)297nADefines magnetic coupling strength
Qubit loop area~10.4 × 10.2µm²Superconducting flux qubit footprint
Aluminum wire width300nmSensitivity-limiting dimension on qubit line
Aluminum film thickness90nmEvaporated superconducting layer
Readout resonator frequency6.95GHzSQUID-based transmission line resonator
Readout interval1µsJosephson bifurcation readout method
Nano-diamond size140nmTypical diameter (NDNV140nmHi10ml)
External bias field (B∥)2.5mTIn-plane magnetization field
Perpendicular bias (B⊥,bias)±10µTQubit frequency tuning (±1/2 Φ₀)
NV center concentration~3ppmIn commercial HPHT nano-diamonds
Parasitic resonance frequency2.023GHzUsed for local nano-diamond heating
Heater power rangeUp to 2.5nWMaximum tested without saturation
Magnetic field sensitivity112pT/√HzAt T = 50 mK base temperature
Temperature sensitivity (50 mK)45.5µK/√HzConverted from B-field sensitivity
Temperature sensitivity (9.1 mK)1.3µK/√HzAt base temperature
Phase relaxation time (T₂)23.5nsAt T = 50 mK
Phase relaxation time (T₂)18.7nsAt T = 9.1 mK
Readout visibility (V)7.88 × 10⁻²—At T = 50 mK measurement
Readout visibility (V)8.24 × 10⁻²—At T = 9.1 mK measurement
Energy splitting (√Δ² + ε²)/h5.227 - 5.261GHzQubit operating energy
Optimal magnetic field (B∥^opt)10.1mTTheoretical sensitivity maximum
Predicted sensitivity gain2.4×—At B∥^opt vs. B∥ = 2.5 mT
Frequency derivative dε/dB⊥95.06GHz·µT⁻¹Determined from qubit parameters
Temperature readout noise< 7.2µKObserved drift over ~5 min intervals
Quantum coherence timescale~100msWhite noise dominant regime
Allan deviation minimum~10s1/f noise crossover frequency
  1. Qubit Fabrication on Silicon Substrate
    • Aluminum evaporation to 90 nm thickness
    • Aluminum wire width patterning: 300 nm
    • Integrated heater line and microwave excitation line
  2. Nano-Diamond Deposition
    • Commercial HPHT nano-diamonds (Adámas NDNV140nmHi10ml)
    • Spread directly onto qubit chip surface
    • Typical particle size: 140 nm
  3. Magnetic Field Configuration
    • In-plane polarizing field: B∥ = 2.5 mT
    • Perpendicular bias field: B⊥,bias ~ 10 µT (order of magnitude)
    • Active cancellation to maintain operating point
  4. Qubit Frequency Characterization
    • Energy gap and persistent current extracted from spectroscopy
    • Coupling to SQUID loop for dispersive readout
  5. Dilution Refrigerator Operation
    • Base temperature: ~10 mK (9.1 mK measured)
    • Measurement stabilization at T = 50 mK for Ramsey studies
    • Local heating via parasitic resonance at 2.023 GHz
  6. Ramsey Interferometry Protocol
    • Quantum superposition prepared via resonant microwave pulse
    • Phase evolution time τ optimized to T₂
    • X-basis readout for coherent state measurement
  7. Sensitivity Calibration
    • Magnetic field sensitivity derived from qubit parameters
    • Temperature sensitivity converted via dB⊥,M/dT⁻¹ slope
    • Validated against RuO and Co nuclear orientation thermometers
  8. Noise Analysis
    • Allan deviation measured from 1 µs to 1 hour
    • Comparison between quantum superposition and ground states
    • Identification of white noise, 1/f noise, and random walk regimes

This research demands precision-engineered nano- and microcrystalline diamond with well-controlled spin defect concentrations for quantum sensing applications. The specific requirements align directly with our portfolio:

Research Requirement6CCVD Material Solution
140 nm nano-diamonds with P1 centersCustom-sized Polycrystalline Diamond (PCD) powders or Single Crystal Diamond (SCD) fragments
HPHT-synthesized diamond with substitutional NOptical Grade SCD with tunable nitrogen incorporation
Strong magnetic coupling to superconducting loopUltra-smooth PCD substrates (Ra &lt; 5 nm) for direct qubit fabrication
High purity for low defect noiseHigh-purity SCD plates grown via MPCVD with &lt; 1 ppm nitrogen
Electron spin polarization at mK temperaturesBoron-Doped Diamond (BDD) or pristine SCD as ordered spin ensemble hosts

The experimental setup requires diamond forms and dimensions beyond off-the-shelf availability. 6CCVD’s flexible manufacturing supports:

  • Custom Particle Synthesis: MPCVD-grown diamond nanoparticles and fragments with controlled size distributions (sub-µm to mm scale) — an alternative to HPHT batches with batch-to-batch variability.
  • Wafer-Scale Integration: PCD plates up to 125 mm diameter enabling multi-qubit array fabrication across a single substrate.
  • Thickness Tailoring: SCD and PCD thickness control from 0.1 µm to 500 µm, plus substrates up to 10 mm thick for robust thermal anchoring in dilution refrigerator environments.
  • Surface Engineering: Sub-nanometer polishing (Ra &lt; 1 nm for SCD, &lt; 5 nm for inch-size PCD) maximizes spin coherence and minimizes qubit decoherence from surface defects.
  • Metallization Stack Customization: Internal Ti/Pt/Au, Ti/W/Au, or other multilayer schemes compatible with superconducting circuit fabrication — including aluminum-compatible interface layers if needed.
  • Laser Cutting & Dicing: Precision shaping of diamond into arbitrary geometries for hybrid quantum device integration.

6CCVD’s in-house PhD-level engineering team provides material consultation for advanced quantum technology projects, including:

  • Defect Concentration Tuning: Guidance on nitrogen incorporation during MPCVD growth to match desired P1/NV center ratios for optimal Curie-law magnetization responses.
  • Surface Chemistry Optimization: Recommendations on terminal group control (hydrogen vs. oxygen termination) to enhance spin coherence times (T₂) in nano-diamond applications.
  • Thermal Anchoring Design: Substrate selection and metallization schemes for cryogenic mounting that minimize parasitic heating and vibration coupling.
  • Quantum Device Prototyping: Collaborative material specification for researchers developing NV-based magnetometers, quantum thermometers, and hybrid superconducting-spin systems.

For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

Abstract Interest is growing in the development of quantum sensing based on the principles of quantum mechanics, such as discrete energy levels, quantum superposition, and quantum entanglement. Superconducting flux qubits are quantum two-level systems whose energy is sensitive to a magnetic field. Therefore, they can be used as high-sensitivity magnetic field sensors that detect the magnetization of a spin ensemble. Since the magnetization depends on temperature and the magnetic field, the temperature can be determined by measuring the magnetization using the flux qubit. In this study, we demonstrated highly sensitive temperature sensing with high spatial resolution as an application of a magnetic field sensor using the quantum coherence of a superconducting flux qubit. By using a superconducting flux qubit to detect the temperature dependence of the polarization ratio of electron spins in nano-diamond particles, we succeeded in measuring the temperature with a sensitivity of 1.3 µ Kµ <mml:math xmlns:mml=“http://www.w3.org/1998/Math/MathML” overflow=“scroll”> <mml:msup> <mml:msqrt> <mml:mrow> <mml:mtext>Hz</mml:mtext> </mml:mrow> </mml:msqrt> <mml:mrow> <mml:mo>−</mml:mo> <mml:mn>1</mml:mn> </mml:mrow> </mml:msup> </mml:math> at T = 9.1 mK in the submicrometer range.