High temperature stability of H-diamond high frequency MOSFET with 300°C grown Al2O3dielectric
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2023-06-13 |
| Journal | Functional Diamond |
| Authors | Ma Yuanchen, Zeyang Ren, YANG SHI-QI, Kai Su, Jinfeng Zhang |
| Institutions | Wuhu Institute of Technology, Xidian University |
| Citations | 4 |
| Analysis | Full AI Review Included |
High Temperature Stability of H-Diamond High Frequency MOSFET with 300°C Grown Al2O3 Dielectric — Technical Documentation
Section titled “High Temperature Stability of H-Diamond High Frequency MOSFET with 300°C Grown Al2O3 Dielectric — Technical Documentation”Executive Summary
Section titled “Executive Summary”- Device Architecture: Hydrogen-terminated (H-diamond) MOSFET fabricated on single-crystal diamond (SCD) substrate using 300°C ALD-grown Al2O3 as both gate dielectric and surface passivation layer.
- Key Geometries: Gate length (Lg) = 100 nm, gate/drain spacing (Lgd) = 2 µm, Al2O3 thickness (tox) = 10 nm, gate width (Wg) = 100 µm.
- Peak DC Performance: Maximum saturation drain current of −492.6 mA/mm and peak transconductance (gm) of 135.2 mS/mm at room temperature.
- High-Temperature Stability: Drain current only decreases by ~7.6% at 200°C (from −492.6 mA/mm to −454.9 mA/mm), with stable threshold voltage (Vth = −4.06 V), validating the thermal robustness of the 300°C ALD Al2O3 process.
- RF Performance: Maximum cut-off frequency (fT) = 36.2 GHz and maximum oscillation frequency (fmax) = 70.5 GHz — among the highest reported for diamond MOSFETs.
- Switching Capability: Transient drain current measurements confirm reliable 1 MHz switching operation, demonstrating feasibility for high-speed power electronics.
- Core Innovation: Demonstrates that 300°C ALD Al2O3 uniquely balances low defect density with the negative interfacial charge needed to sustain the 2D hole gas (2DHG) layer, enabling both high-frequency and high-temperature operation simultaneously.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context / Condition |
|---|---|---|---|
| Substrate Material | Single-Crystal Diamond (SCD) | — | (001) orientation, CVD-grown |
| Surface Termination | Hydrogen-terminated (H-diamond) | — | Forms 2DHG surface conductive layer |
| Gate Dielectric | Al2O3 | — | Grown by ALD at 300°C |
| Dielectric Thickness (tox) | 10 | nm | Atomic Layer Deposition |
| Gate Length (Lg) | 100 | nm | Sub-micron RF geometry |
| Gate/Drain Spacing (Lgd) | 2 | µm | Access region |
| Source/Drain Spacing (Lsd) | 0.5 | µm | Access region |
| Gate Width (Wg) | 100 | µm | Two-finger configuration |
| Maximum Saturation Drain Current (IDmax) | −492.6 | mA/mm | Room temperature (26°C) |
| IDmax at 200°C | −454.9 | mA/mm | Only 7.6% degradation |
| Peak Transconductance (gm) | 135.2 | mS/mm | At room temperature |
| Threshold Voltage (Vth) | −4.06 | V | Negative for p-channel operation |
| Maximum Oscillation Voltage Swing | ±1.3 | V | Measured at Vpp |
| Cut-off Frequency (fT) | 36.2 | GHz | Maximum reported |
| Maximum Oscillation Frequency (fmax) | 70.5 | GHz | Maximum reported |
| Switching Response | 1 | MHz | Verified transient pulse response |
| Diamond Bandgap | 5.47 | eV | Wide-bandgap semiconductor |
| Hole Mobility (diamond) | 3800 | cm2 V−1 s−1 | High carrier mobility |
| Thermal Conductivity (diamond) | 2200 | W/m·K | Excellent heat dissipation |
| Breakdown Field (diamond) | >10 | MV/cm | High-power capability |
Key Methodologies
Section titled “Key Methodologies”- Substrate Preparation: Single-crystal CVD diamond substrate prepared with hydrogen-terminated surface to induce a 2D hole gas (2DHG) layer responsible for surface conductivity.
- Ohmic Contact Formation: Au (gold) metallization for source and drain electrodes — standard non-alloyed ohmic scheme for H-diamond.
- Gate Dielectric Deposition: Al2O3 grown by Atomic Layer Deposition (ALD) at 300°C, used as both gate oxide and surface passivation — the moderate growth temperature preserves hydrogen termination while suppressing interfacial defects.
- Device Patterning: Sub-micron gate lithography yielding Lg = 100 nm and Lgd = 2 µm for high-frequency operation.
- DC Characterization: ID-VDS and ID-VGS sweeps at 26°C and 200°C to assess thermal stability.
- RF Characterization: S-parameter extraction to determine fT and fmax.
- Transient Switching Test: Pulsed gate drive at 1 MHz to evaluate high-speed switching fidelity.
- Interfacial Analysis (Prior Work): XPS band-offset measurements confirming negative fixed charge in Al2O3 that attracts holes to the H-diamond interface and stabilizes the 2DHG.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”-
Applicable Materials:
- Optical/Electronic Grade SCD (Single-Crystal Diamond): This paper relies explicitly on single-crystal diamond (001) substrates. 6CCVD supplies high-purity MPCVD-grown SCD with exceptional crystalline quality, the ideal foundation for 2DHG devices requiring low defect density at the interface.
- Surface Termination: 6CCVD provides hydrogen-terminated SCD and PCD surfaces engineered to yield robust 2DHG layers compatible with subsequent ALD deposition.
-
Customization Potential:
- Dimensional Control: 6CCVD plates and wafers up to 125 mm (PCD) and SCD substrates in custom thicknesses ranging from 0.1 µm to 500 µm allow flexibility for both lateral MOSFET geometries and novel vertical architectures.
- Laser Cutting & Dicing: Sub-micron gate definition requires precisely dimensioned substrates; 6CCVD offers custom laser cutting to deliver die sizes matched to your lithographic layout.
- Metallization Services: 6CCVD’s in-house metalization capabilities cover Au, Pt, Pd, Ti, W, and Cu. The Au source/drain contacts used in this study are a standard 6CCVD offering, and Ti/Au or other stacks are available for thermal stability or wire-bonding optimization.
- Ultra-Smooth Surfaces: For ALD-Al2O3 deposition, surface roughness directly impacts gate leakage and threshold voltage stability. 6CCVD delivers SCD polished to Ra < 1 nm, ensuring uniform 10 nm dielectric integrity and reproducible Vth.
-
Engineering Support:
- 6CCVD’s in-house PhD engineering team is available to assist with material selection, surface preparation protocols, and dielectric integration for high-frequency diamond MOSFET, high-temperature power electronics, and RF power amplifier projects.
- Whether your application targets 36 GHz RF operation, 200°C+ thermal environments, or fast-switching power conversion, 6CCVD can recommend the appropriate SCD/PCD grade and surface treatment to extend the results reported here.
-
Call to Action: For custom specifications, material consultation, or metallization guidance for your diamond MOSFET program, visit 6ccvd.com or contact our engineering team directly.
View Original Abstract
The high frequency H-diamond metal-oxide-semiconductor field effect transistors (MOSFETs) were fabricated on single diamond substrate using 300°C ALD grown Al2O3 as gate dielectric and passivation layer. The devices gate length, gate/drain spacing and dielectric thickness are 100 nm, 2 μm, and 10 nm, respectively. The direct-current and frequency characteristics were investigated. The device shows a maximum saturation drain current of −492.6 mA/mm and gm of 135.2 mS/mm. The device shows good high temperature working performance, and the maximum saturation drain current only has a little decreasing of 7.6%. at 200°C. In addition, the device exhibits a maximum cut-off frequency of 36.2 GHz and maximum oscillation frequency of 70.5 GHz. The transient drain current response measurement indicates that the drain current can follow the changing of gate voltage at the frequency of 1 MHz. These results indicate that the Al2O3 dielectric is suitable for using in high frequency or the high-speed switching devices.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2003 - Surface band bending and surface conductivity of hydrogenated diamond