Method and article of manufacture corresponding to a composite comprised of ultra nonacrystalline diamond, metal, and other nanocarbons useful for thermoelectric and other applications

MetadataDetails
Publication Date2023-05-10
JournalOSTI OAI (U.S. Department of Energy Office of Scientific and Technical Information)
AuthorsD. M. Gruen
AnalysisFull AI Review Included
  • Material Innovation: Patent US 7,718,000 B2 describes a composite material combining ultra-nanocrystalline diamond (UNCD) powder (crystallites sized 2-10 nm) with metallic components (cobalt, nickel, iron, etc.) to produce encapsulated nanowires or quantum dots.
  • Thermoelectric Goal: The primary objective is achieving a high figure of merit (ZT) by maximizing electrical conductivity and Seebeck coefficient while minimizing thermal conductivity — a combination historically difficult in bulk materials.
  • Manufacturing Process: UNCD powder is mixed with metal salts in aqueous solution, optionally with polymeric adhesives (polymethacrylate, polyvinylpyrrolidone), then heated in a reducing atmosphere (H2/CH4) at ≥600°C (up to 800°C) to reduce metals and form carbon-encapsulated nanostructures.
  • Structural Outcome: The resulting composite exhibits high electrical conductivity, low thermal conductivity, mechanical rigidity, and stability up to 1000°C, with density approximately one-third to one-half that of bulk diamond.
  • Targeted Applications: Thermoelectric power generation, pebble-bed nuclear reactor fuel/cladding, and radiation-based targeted cancer therapy delivery systems.
  • Key Advantage: The process allows inhomogeneous metal concentration distribution, enabling gradient doping between hot and cold terminuses of thermoelectric devices for optimized p-n junction performance.
  • Scalable Form Factors: Because the diamond component begins as a powder, arbitrary shapes and sizes can be produced to meet specific device geometries.
ParameterValueUnitContext
UNCD crystallite size2-10nmPrimary particle dimension of disperse diamond powder
Target crystallite maximum≤10nmUpper bound for “ultra-nanocrystalline” classification
Surface area (UNCD powder)500-1000m2/gHigh surface area enabling dense metal salt absorption
Cobalt nitrate concentration5-10mol/LAqueous solution saturation range
Preferred cobalt concentration5molarExample concentration in water
Stoichiometry goal~1 Co atom per surface C atomratioSaturation absorption target
Reaction temperature≥600 (up to 800)°CMinimum temperature for salt reduction and reaction initiation
Reducing atmosphereH2 + CH4—Composition for metal ion reduction
Resultant material thermal stabilityUp to 1000°CMaximum operating temperature
Density (final composite)1/3 to 1/2 of bulk diamondrelativeLower than diamond due to nanoporosity
Initial paste density~1.0g/cm3After metal salt absorption
Target ZT figure of merit≥4 (ideal)dimensionlessCompared to state-of-the-art ~1 for Bi2Te3-Bi2Se3 or Si-Ge alloys
Typical TE conversion efficiency (prior art)5-10 (max ~14)%Baseline performance benchmark
Encapsulation typesFullerenes, graphite, MWCNTs—Carbon shell structures formed during reaction
Adhesive optionsPolymethacrylate, polyvinylpyrrolidone—Mechanical integrity enhancers
Applicable metal systems3D, 4D, 5D, 4F, 5F series; Co, Fe, Ni, Cu, Mn, U, Pu, Eu, Gd—Periodic table groupings suitable for reaction
  • Provision of UNCD Powder: Source ultra-nanocrystalline diamond material with crystallite sizes between 2-10 nm, typically produced via detonation synthesis techniques.
  • Preparation of Metal Salt Solution: Dissolve metal salt (e.g., cobalt nitrate) in water at 5-10 mol/L concentration to achieve high solubility and saturation absorption.
  • Mixing with Optional Adhesive: Combine UNCD crystallites with metal salt solution, optionally adding polymethacrylate and polyvinylpyrrolidone as water-based adhesives to enhance coating mechanical integrity.
  • Surface Absorption Phase: Allow the aqueous mixture to reach a paste-like consistency where approximately one metal atom is absorbed per exposed surface carbon atom (leveraging 500-1000 m2/g surface area).
  • Aqueous Removal (Heating Stage 1): Heat the solution to ≥600°C (typically 700-800°C) in a reducing atmosphere to evaporate water content.
  • Reduction Reaction (Heating Stage 2): Maintain reducing atmosphere of H2 and CH4 to reduce metal ions from salt to pure metallic state.
  • Nanostructure Formation: During reduction, cobalt (or alternative metal) catalyzes nanotube growth while simultaneously forming carbon-encapsulated nanowires and quantum dots (fullerenic, graphitic, or MWCNT shells).
  • Inhomogeneous Doping (Optional): Combine crystallites with multiple metal salts at varying concentrations to produce gradient metal concentration between hot and cold terminuses of the thermoelectric element.
  • Shape Forming: While the material remains in powder/paste form, shape into desired geometric configurations before final densification.
  • Quality Verification: Confirm thermal stability (up to 1000°C), electrical conductivity, and low thermal conductivity of the final composite.

The research outlined in this patent relies on ultra-nanocrystalline diamond (UNCD) powder as a foundational feedstock material, followed by complex metal-salt impregnation and high-temperature reduction processing. While 6CCVD specializes in MPCVD-grown diamond plates and wafers rather than detonation-synthesized UNCD powders, our capabilities directly support the downstream device fabrication, metallization, and integration stages required to translate this research into functional thermoelectric, nuclear, and biomedical devices.

6CCVD ProductRelevance to UNCD Composite Research
Single Crystal Diamond (SCD) WafersUltra-smooth Ra < 1nm polished SCD substrates serve as ideal test beds and heat-spreader interfaces for thermoelectric device characterization.
Polycrystalline Diamond (PCD) PlatesInch-size PCD with Ra < 5nm polish provides mechanically rigid, thermally conductive platforms for mounting UNCD-metal composite legs in p-n junction configurations.
Boron-Doped Diamond (BDD)Conductive BDD electrodes (available in custom doping levels) can serve as charge-collecting contacts for thermoelectric generators and electrochemical sensing applications.
Optical Grade SCDOptical-grade substrates enable in-situ Raman and photoluminescence characterization of UNCD-metal composite films during device operation.
  • Custom Metallization: The patent requires intimate electrical contact between carbon-encapsulated metal nanowires and external circuitry. 6CCVD offers in-house metallization with Au, Pt, Pd, Ti, W, and Cu, enabling tailored ohmic or Schottky contact formation directly onto diamond substrates and composite interfaces.
  • Precision Laser Cutting: Thermoelectric generator legs and nuclear fuel pellets require specific form factors. Our laser cutting services can produce custom geometries from PCD plates (up to 125mm) and SCD wafers for integration into prototype devices.
  • Thickness Control: For membrane-based or thin-film thermoelectric architectures, 6CCVD provides SCD and PCD films in thicknesses from 0.1µm to 500µm, as well as bulk substrates up to 10mm thick for structural support layers.
  • Boron Doping Tuning: Custom BDD doping concentrations allow engineers to match the work function and electrical conductivity of diamond contacts to the specific metal-carbide nanowire composites developed through this UNCD process.

6CCVD’s in-house PhD team can assist with:

  • Material selection guidance for thermoelectric device substrate and contact layers
  • Thermal interface engineering using high-conductivity PCD heat spreaders
  • Metallization stack design (e.g., Ti/Pt/Au or Cr/Pd/Au) for reliable wire bonding or soldering to UNCD-metal composite elements
  • Surface preparation protocols to maximize adhesion between UNCD composites and diamond substrates
  • Co-development of custom geometries for pebble-bed reactor cladding prototypes or biomedical radiation-delivery platforms

For researchers replicating or extending the thermoelectric power generation work described in this patent, 6CCVD recommends pairing UNCD-metal composite legs with our polished PCD or SCD substrates featuring custom Ti/W metallization for high-temperature stable contacts. The thermal stability window of our diamond products (functioning reliably above 1000°C in inert atmospheres) aligns well with the operating envelope specified in the patent.

For pebble-bed nuclear reactor applications, our BDD and undoped PCD spheres or pellets (custom-cut from larger plates) can serve as baseline cladding materials for comparative testing against the UNCD composites disclosed herein.

For radiation-based cancer treatment delivery systems, our ultra-smooth SCD wafers (Ra < 1nm) provide biocompatible substrates for composite immobilization and in-vitro characterization.

For custom specifications, metallization stack design, or material consultation regarding diamond substrates and contacts for thermoelectric, nuclear, or biomedical composite applications, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

One provides (101) disperse ultra-nanocrystalline diamond powder material that comprises a plurality of substantially ordered crystallites that are each sized no larger than about 10 nanometers. One then reacts (102) these crystallites with a metallic component. The resultant nanowire is then able to exhibit a desired increase with respect to its ability to conduct electricity while also substantially preserving the thermal conductivity behavior of the disperse ultra-nanocrystalline diamond powder material. The reaction process can comprise combining (201) the crystallites with one or more metal salts in an aqueous solution and then heating (203) that aqueous solution to remove the water. This heating can occur in a reducing atmosphere (comprising, for example, hydrogen and/or methane) to also reduce the salt to metal.