Skip to content

Cross‐Correlated Quantum Thermometry Using Diamond Containing Dual‐Defect Centers

MetadataDetails
Publication Date2023-09-10
JournalAdvanced Sensor Research
AuthorsMadhav Gupta, Tongtong Zhang, Lambert Yeung, Jiahua Zhang, Yayin Tan
InstitutionsSichuan University, Dongguan University of Technology
Citations4
AnalysisFull AI Review Included
  • Dual-defect quantum thermometry: First-ever demonstration of simultaneous, cross-validated temperature sensing in a single bulk diamond co-doped with Nitrogen-Vacancy (NV) and Silicon-Vacancy (SiV) centers.
  • Complementary modalities: NV centers enable high-sensitivity spin-based (ODMR) readout (22 mK·√Hz-1), while SiV centers provide an artefact-immune all-optical (PL) readout (86 mK·√Hz-1) — both interrogated in the same sample.
  • Cross-validation under artefacts: A perfect linear correlation between NV-ODMR frequency shift and SiV zero-phonon line (ZPL) shift permits real-time validation, even in the presence of dynamic magnetic fields (40 G).
  • Biological relevance: SiV emission at 737 nm falls within the near-infrared biological transparency window, making the platform directly applicable to in-vivo and intracellular thermometry.
  • Single-platform architecture: Unlike previous dual-mode approaches using physically separated nanodiamonds and UCNPs, both defects are embedded in one bulk host — preserving spatial and temporal co-localization.
  • Proof-of-concept milestone: Establishes a new reliability standard for quantum thermometry in complex electromagnetic environments (e.g., neuron cells, integrated electronics).
ParameterValueUnitContext
NV-ODMR temperature sensitivity22mK·√Hz-1Spin-based readout
SiV-PL temperature sensitivity86mK·√Hz-1All-optical readout
NV Zero-Field Splitting (D)≈2.87GHzRoom temperature baseline
NV-ODMR frequency shift (dD/dT)-73.79kHz/°CLinear fit
SiV ZPL position (25 °C)737nm1.68 eV
SiV ZPL thermal shift (dλ/dT)0.0398nm/°CLinear fit
SiV ZPL linewidth (FWHM)≈4.8nmRoom temp, ensemble
NV ZPL linewidth (FWHM)≈3nmRoom temp, ensemble
SiV ZPL FWHM thermal shift0.0084nm/°CBroadening rate
SiV Debye-Waller Factor≈0.7—Fraction of emission in ZPL
NV Debye-Waller Factor0.04—Fraction of emission in ZPL
SiV ground-state spin-orbit splitting≈50GHzIntrinsic
SiV spin quantum numberS = 1/2—Electron spin
CW-ODMR linewidth12MHzEnsemble measurement
ODMR contrast11.74%25 °C
Excitation wavelength532nmPL and ODMR pump
Operating temperature range27-48°CTested window
Dynamic B-field amplitude40GArtefact test condition
SiV photostability deviation0.41%Over measurement duration
Cross-validation sensitivity (ZPL vs D)-0.548nm/MHzDual-mode linkage
Cross-validation sensitivity (FWHM vs D)-0.114nm/MHzDual-mode linkage
  • Sample platform: Bulk single-crystal diamond (1b-type) co-doped with nitrogen (for NV formation) and silicon (for SiV formation) via in-situ doping during CVD growth.
  • Optical characterization: Custom-built wide-field quantum diamond microscope (see Supporting Information Fig. S1) used for both PL and CW-ODMR mapping.
  • PL spectroscopy: 532 nm laser excitation; ZPL peaks identified at 637 nm (NV) and 737 nm (SiV); Lorentzian fitting extracts peak position and linewidth.
  • ODMR readout: Continuous-wave ODMR at zero-field splitting around 2.87 GHz; resonance frequency tracked vs. temperature for thermometry.
  • Temperature calibration: Sample stage swept between 27 °C and 48 °C; both modalities recorded simultaneously to establish linear cross-calibration.
  • Artefact test: External dynamic magnetic field of 40 G applied to demonstrate immunity of SiV readout and need for NV cross-validation (and vice versa).
  • Data correlation: NV-ODMR frequency, SiV ZPL position, and SiV FWHM fitted with linear regressions; cross-sensitivity coefficients extracted for real-time validation.
  • Noise-floor extraction: Shot-noise-limited sensitivity derived from integration-time sweeps for both modalities.
Research RequirementRecommended 6CCVD Product
Co-doped bulk diamond with NV + SiV centersCustom Co-Doped Single Crystal Diamond (SCD) — controlled N and Si incorporation during MPCVD growth
High optical-grade host for ZPL analysisOptical Grade SCD — Ra < 1 nm polished surfaces minimize scattering at 637 nm and 737 nm
Large-area, low-birefringence host for wide-field microscopySCD Plates/Wafers up to 125 mm (PCD equivalent available; SCD sizes confirmed upon request)
Thickness tuning for transmission vs. confocal geometrySCD Thickness Range 0.1 µm - 500 µm
  • Tailored co-doping profiles: 6CCVD MPCVD reactors allow precise control of N and Si precursor flows, enabling tunable NV and SiV ensemble densities for optimized signal-to-noise in quantum sensing.
  • Custom metalization for device integration: Ti, Pt, Au, Pd, W, and Cu deposition available in-house — useful for integrating microwave striplines (for ODMR drive) or microheaters (for in-situ calibration) directly on the diamond.
  • Laser cutting & dicing: Custom geometries (membranes, micro-discs, patterned arrays) supported for miniaturized sensor packages or fiber-coupled probes.
  • Surface polishing: Sub-nanometer Ra finishes on SCD preserve ZPL spectral purity by reducing surface-related luminescence background.
  • Substrate options: For hybrid integration with photonic or electronic chips, diamond substrates up to 10 mm thickness are available.
  • PhD-led consultation: 6CCVD’s in-house materials science team can advise on defect engineering — including target NV/SiV concentration ratios, post-growth annealing recipes, and surface passivation strategies — to replicate or extend this dual-defect thermometry platform.
  • Application-specific guidance: Whether the end use is intracellular nanothermometry, on-chip thermal mapping of microelectronics, or quantum-enhanced metrology, our engineers can recommend the optimal material grade and geometry.
  • Rapid prototyping: Custom geometries and doping specifications can be quoted with short lead times for research-scale quantities.

Call to Action: For custom specifications or material consultation, visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

Abstract The contactless temperature measurement at micro/nanoscale is vital to a broad range of fields in modern science and technology. The nitrogen‐vacancy (NV) center, a kind of diamond defect with unique spin‐dependent photoluminescence, is recognized as one of the most promising nanothermometers. However, this quantum thermometry technique is prone to a number of possible perturbations, which will unavoidably degrade its actual temperature sensitivity. Here, for the first time, a cross‐validated optical thermometry method is developed using a bulk diamond sample containing both NV centers and silicon‐vacancy (SiV) centers, achieving a sensitivity of 22 and 86 mK (√Hz) −1 respectively. Particularly, the latter has been intrinsically immune to those influencing perturbations for the NV‐based quantum thermometry, hence serving as a real‐time cross‐validation system. As a proof‐of‐concept demonstration, a trustworthy temperature measurement is shown under the influence of varying magnetic fields, which is a common artefact present in practical systems. This multi‐modality approach allows synchronized cross‐validation of the measured temperature, which is required for micro/nanoscale quantum thermometry in complicated environments such as a living cell.