Diamond Compact Electrodes with Increased Electroactivity - Anodic Oxidation of Ethylenediaminetetraacetic Acid

MetadataDetails
Publication Date2023-09-01
JournalЭлектрохимия
AuthorsYu. V. Pleskov, M. D. Кrotova, Е. А. Екимов
InstitutionsFrumkin Institute of Physical Chemistry and Electrochemistry, Institute for High Pressure Physics

The diamond electrodes-compacts with extreme high boron-doping level, added with platinum, were prepared at a pressure of 8―9 GPa and temperature ~2500 К from growth mixtures В-С, Pt-C, and Pt-C-B. They are highly electroactive in the reaction of ethylenediaminetetraacetic acid electrooxidation. The oxidation current is a linear function of the ethylenediaminetetraacetic acid concentration over the 0.001-0.05 g-equ/L range. This system can be basic to an electroanalytical method for the ethylenediaminetetraacetic acid determination.