Laser and Ion Beam Writing for Quantum Photonic Sensors in Diamond
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2025-01-01 |
| Authors | Ottavia Jedrkiewicz, Vibhav Bharadwaj, Alina C. Kuriakose, Giulio Coccia, Francesco P. Mezzapesa |
Abstract
Section titled āAbstractāUltrafast laser writing and Ion beam writing have emerged as valuable techniques for fabricating building-blocks of photonic and sensing diamond platforms. These techniques can be used to form quantum emitters, waveguides, microchannels and conductive microwires.