Angular dependent terahertz emission from the interplay between nanocrystal diamond film and plasmonic metasurface

MetadataDetails
Publication Date2024-01-21
JournaliScience
AuthorsShuangquan Fang, Wenpeng Guo, Yuanyuan Huang, Mingjian Shi, Xuezeng Tian
InstitutionsUniversity of Chinese Academy of Sciences, Songshan Lake Materials Laboratory
Citations2

Composite structures integrated with metasurfaces and nonlinear films have emerged as alternative candidates to enhance nonlinear response. The cooperative interaction between the two components is complicated. Herein, a split-ring resonator (SRR)-type metasurface was fabricated on a free-standing nanocrystal diamond (NCD) film utilizing electron beam lithography, electron beam evaporation, and a lift-off process. The terahertz (THz) radiation from the SRR-NCD under normal incidence originates from the high-order magnetic resonance of SRR because the NCD film cannot produce detectable THz radiation at this incident angle. As increasing the incident angle, the contribution of the THz radiation from the NCD film gradually increases until reaching 40° incident angle limitation. The results indicate that this angular-dependent THz radiation is induced by the interplay between the NCD film and SRR. This study offers a new approach to investigate nonlinear processes in composite structures.

  1. 2012 - A roadmap for graphene [Crossref]
  2. 2014 - Plasmon Enhanced Terahertz Emission from Single Layer Graphene [Crossref]
  3. 2018 - Terahertz Surface Emission from Layered MoS2 Crystal: Competition between Surface Optical Rectification and Surface Photocurrent Surge [Crossref]
  4. 2020 - Terahertz emission from in-plane and out-of-plane dipoles in layered SnS2 crystal [Crossref]
  5. 2022 - Interplay between Ultrafast Shift Current and Ultrafast Photon Drag Current in Tellurium Nanotubes [Crossref]
  6. 2014 - Mechanisms of THz generation from silver nanoparticle and nanohole arrays illuminated by 100Ā fs pulses of infrared light [Crossref]
  7. 2011 - THz Generation from Plasmonic Nanoparticle Arrays [Crossref]
  8. 2021 - Functional THz emitters based on Pancharatnam-Berry phase nonlinear metasurfaces [Crossref]
  9. 2014 - Broadband terahertz generation from metamaterials [Crossref]
  10. 2020 - Nonlinear Plasmonic Metasurface Terahertz Emitters for Compact Terahertz Spectroscopy Systems [Crossref]