Intravital microscopic thermometry of rat mammary epithelium by fluorescent nanodiamond

MetadataDetails
Publication Date2024-01-01
JournalNanoscale Horizons
AuthorsTakahiro Hamoya, Kiichi Kaminaga, Ryuji Igarashi, Yukiko Nishimura, Hiromi Yanagihara
InstitutionsKyoto Prefectural University of Medicine, Tokyo Institute of Technology
Citations4

This study reports an application of microscopic thermometry in a living rat using quantum sensing based on the fluorescent nanodiamond (FND) nitrogen-vacancy center, demonstrating the relevance of the technique in biomedical research using a mammal.