Perfectly-aligned diamond quantum sensors to visualize superconducting vortices
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-01-01 |
| Authors | Shunsuke Nishimura, Taku Kobayashi, Kensuke Ogawa, Takeyuki Tsuji, Takayuki Iwasaki |
Abstract
Section titled āAbstractāWe present a wide-field imaging technique using perfectly-aligned diamond quantum sensors to accurately visualize superconducting vortices in a thin film. Our results agree with theoretical models, validating our methodās precision and versatility in characterizing superconductors.