Photoinduced Modification of Second Harmonic Generation in Diamond Cavities

MetadataDetails
Publication Date2024-01-01
AuthorsSigurd FlƄgan, Joe Itoi, Prasoon K. Shandilya, Elham Zohari, Vinaya Kumar Kavatamane

We demonstrate cavity-enhanced second-harmonic generation from a diamond microdisk. By performing multicolor illumination, we show that optical manipulation of nitrogen-vacancy centers strongly affects the second-harmonic signal, indicating a difference in χ (2) between two possible electronic configurations.