Ultra-low AC Susceptibility Measurement with Quantum Diamond Microscope

MetadataDetails
Publication Date2024-01-01
AuthorsDasika Shishir, Kasturi Saha

Conventional AC susceptometers are limited to measuring AC susceptibilities oF the order of nJT āˆ’1 . In this study, we showcase the application of a diamond quantum magnetometer and dynamical control sequences to assess susceptibilities in Permalloy micro-disks at magnitudes as low as a few fJT āˆ’1 .