Optimal concentration of holes and electrons in semiconductors for energy harvesting based on love waves propagation in a PSC film/substrate
At a Glance
Section titled âAt a Glanceâ| Metadata | Details |
|---|---|
| Publication Date | 2024-03-15 |
| Journal | Materials Today Sustainability |
| Authors | Houda Boukhriss, Issam Ben Salah, Anouar Njeh, Farid Takali, Cherif Othmani |
| Institutions | University of Sfax, Technische Universität Dresden |
| Citations | 8 |
Abstract
Section titled âAbstractâPublished papers on the topic of acoustic waves in piezoelectric semiconductor (PSC) material often deal separately with the concentrations of holes and electrons. The only exception is a recent published results by (Zhu et al., 2018), which addressed the problem using two values p0=2Ă1024mâ3 and n0=1.2Ă1023mâ3 of p-type semiconductor. However, when considering the both parameters p0 and n0, we need to think about an accurate balance of the concentration of holes and electrons in terms of the energy harvesting issue. Actually, in certain values of p0 and n0 the different phenomena related to the piezoelectric semiconductor properties are disappear, where the PSC material behaves like a purely elastic medium. To this end, we addressed this issue by calculating dispersion curves, mechanical displacement, electric potential, concentrations of holes and electrons under several values of p0 and n0, which has not been addressed in previous works. In comparison to the work of (Zhu et al., 2018), we shift attention from SH modes to the characteristics of Love waves in PSC-ZnO/Diamond. From a technological point of view, surface Love waves can be more convenient than SH modes in nanogenerator applications because they propagate along the surface of the half-space, which allows for significant interaction between the wave and the substrate. From a numerical point of view, we gain the freedom to extend the simplified version of the ordinary differential equation (ODE) method used by (Ben Salah et al., 2022) to consider the PSC-ZnO/Diamond heterostructure. We demonstrate how effective the p0 and n0 values are on the improvement of the distributions of electric potential in accordance with âScreening effectâ. The key observation here is that the Screening effect can provide an overview of energy harvesting. Strictly speaking, the x1-region from 1.57 Îźm to 2.35 Îźm for p-type semiconductor denotes the desired zone, where the electric potential of the PSC structure is positive and the concentration of holes is higher than normal level. However, the negative electrons are clearly associated with this critical x1-region. This observation can be highlighted by a comparison of the distributions and magnitudes of the electric potentials between the piezoelectric and PSC cases. On the other hand, it was found that the values of p0 and n0 can also affect the cut-off frequency of Love waves. However, we discuss the optimal values of p0 and n0 for minimizing the attenuation coefficient.
Tech Support
Section titled âTech SupportâOriginal Source
Section titled âOriginal SourceâReferences
Section titled âReferencesâ- 2022 - SH waves in a stressed piezoelectric semiconductor plates: electron and hole drift phenomenon
- 2018 - Study on the influence of semiconductive property for the improvement of nanogenerator by wave mode approach [Crossref]
- 1962 - Elastic wave propagation in piezoelectric semiconductors [Crossref]
- 2009 - Fundamentals of zinc oxide as a semiconductor [Crossref]
- 2012 - Energy harvesting based on semiconducting piezoelectric ZnO nanostructures [Crossref]
- 2012 - Progress in piezotronics and piezo-phototronics [Crossref]
- 2007 - Nanowire piezoelectric nanogenerators on plastic substrates as flexible power sources for nanodevices [Crossref]
- 2017 - Enhanced performance of a gan piezoelectric nanogenerator with an embedded nanoporous layer via the suppressed carrier screening Effect [Crossref]
- 2018 - Photoactive piezoelectric energy harvester driven by antimony sulfoiodide (SbSI): a AVBVICVII class ferroelectric-semiconductor compound [Crossref]