Analysis of Subsurface Damage Structures of Gallium Nitride Substrates Induced by Mechanical Polishing with Diamond Abrasives
At a Glance
Section titled āAt a Glanceā| Metadata | Details |
|---|---|
| Publication Date | 2024-07-04 |
| Journal | physica status solidi (b) |
| Authors | Natsuko Omiya, Hideo Aida, Hidetoshi Takeda, Motoki Kanda, Toshiro Doi |
| Institutions | Kyushu University, Nagaoka University of Technology |
| Citations | 3 |
Abstract
Section titled āAbstractāSubsurface damage (SSD) structures induced by mechanical polishing of gallium nitride (GaN) substrates are comprehensively investigated using atomic force microscopy, cathodoluminescence (CL) imaging, and crossāsectional transmittance electron microscopy. The low removal rate of the CMP process is a barrier to high productivity of a GaN wafering process; therefore, reducing the chemical mechanical polishing (CMP) process time by reducing the depth of SSD induced by mechanical processing is an active research area. To better understand the SSD structures, the surface roughness, SSD depth, and SSD distributions induced by mechanical polishing are quantitatively evaluated in this study. The SSD structures induced by mechanical polishing can be quantitatively exhibited as the SSD distribution with the damage strength at the outermost surface and the damage propagation, which are obtained by CMP process timeāresolved CL imaging method. On the basis of the analysis results, a schematic model of the SSD structures for mechanically polished GaN substrates is proposed.