Studying critical parameters of superconductor via diamond quantum sensors
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2025-01-27 |
| Journal | New Journal of Physics |
| Authors | Kin On Ho, Wai Kuen Leung, Yiu Yung Pang, King Yau Yip, Jianyu Xie |
| Citations | 2 |
Abstract
Section titled “Abstract”Abstract Critical parameters are the key to superconductivity research, and reliable instrumentations can facilitate the study. Traditionally, one has to use several different measurement techniques to measure critical parameters separately. In this work, we develop the use of a single species of quantum sensor to determine and estimate several critical parameters with the help of independent simulation data. We utilize the nitrogen-vacancy (NV) center in the diamond, which recently emerged as a promising candidate for probing exotic features in condensed matter physics. The non-invasive and highly stable nature provides extraordinary opportunities to solve scientific problems in various systems. Using a high-quality single-crystalline YBa 2 Cu 4 O 8 (YBCO) as a platform, we demonstrate the use of diamond particles and a bulk diamond to probe the Meissner effect. The evolution of the vector magnetic field, the H − T phase diagram, and the map of fluorescence contour are studied via NV sensing. Our results reveal different critical parameters, including lower critical field <mml:math xmlns:mml=“http://www.w3.org/1998/Math/MathML” overflow=“scroll”> <mml:mrow> <mml:msub> <mml:mi>H</mml:mi> <mml:mrow> <mml:mi>c</mml:mi> <mml:mn>1</mml:mn> </mml:mrow> </mml:msub> </mml:mrow> </mml:math> , upper critical field <mml:math xmlns:mml=“http://www.w3.org/1998/Math/MathML” overflow=“scroll”> <mml:mrow> <mml:msub> <mml:mi>H</mml:mi> <mml:mrow> <mml:mi>c</mml:mi> <mml:mn>2</mml:mn> </mml:mrow> </mml:msub> </mml:mrow> </mml:math> , and critical current density j c , as well as verifying the unconventional nature of this high-temperature superconductor YBCO. Therefore, NV-based quantum sensing techniques have huge potential in condensed matter research.