Design a novel rectangular MPCVD reactor operated at 2.45 GHz for diamond growth - A simulation-based study
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2025-06-01 |
| Journal | AIP Advances |
| Authors | Caijie Zhang, Kai Wang, Shixian Cai, Tingru Zhu, Jie Li |
| Institutions | Peking University, State Key Laboratory of Nuclear Physics and Technology |
| Citations | 1 |
Abstract
Section titled “Abstract”The electric field distribution within a microwave plasma chemical vapor deposition (MPCVD) reactor determines the quality of synthetic diamonds. In this study, we aimed to facilitate diamond deposition for various demands by designing a rectangular MPCVD reactor that can balance and regulate the electric field intensity and uniformity in the deposition region. Establishing and utilizing a 3D numerical model, we analyzed the electromagnetic field and plasma distributions of three reactor candidates. One promising candidate was optimized and compared with two cylindrical cavities, each having a diameter equal to the width and diagonal length of the rectangular cavity, respectively. The optimized rectangular reactor combined the TM011, TM021, and TM031 modes, exhibited a high-intensity and uniform electric field in the deposition region without other hot-spot regions, and demonstrated high-density plasma and uniform gas distribution. Operating at 2.45 GHz, the reactor generated a maximum electric field intensity of 2 × 105 V/m, and the hydrogen plasma reached a maximum electron density of 5.9 × 1017 m−3 over an effective area of 4.0 × 103 mm2 at 5 kW power and 20 kPa pressure. These findings highlight the potential of the rectangular reactor design, which exhibits a novel microwave modes coupling mechanism, enabling redistribution of microwave energy, and achieves higher electric field intensity in the deposition region compared with traditional cylindrical reactors. The study emphasizes the significance of the rectangular reactor for the growth of demand-specific diamonds.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2009 - Chemical vapour deposition synthetic diamond: Materials, technology and applications [Crossref]
- 2007 - High quality MPACVD diamond single crystal growth: High microwave power density regime [Crossref]
- 2009 - Understanding the chemical vapor deposition of diamond: Recent progress [Crossref]
- 2021 - Design of an edge tapered 915 MHz/TM021 microwave plasma reactor by numerical analysis [Crossref]
- 2006 - Simulation of temperature and gas flow distributions in region close to a diamond substrate with finite thickness [Crossref]
- 2009 - Microwave engineering of plasma-assisted CVD reactors for diamond deposition [Crossref]
- **** - Microwave plasma reactor
- 1999 - Simulation and development of optimized microwave plasma reactors for diamond deposition [Crossref]
- 1995 - Numerical simulations of microwave plasma reactors for diamond CVD [Crossref]
- 1995 - Modelling the electromagnetic field and plasma discharge in a microwave plasma diamond deposition reactor [Crossref]