Skip to content

Over 450 V breakdown voltage in diamond vertical Schottky barrier diodes with anodic self-aligned mesa termination

MetadataDetails
Publication Date2025-07-21
JournalApplied Physics Letters
AuthorsXixiang Zhao, Shumiao Zhang, Guoqing Shao, Qi Li, Genqiang Chen
InstitutionsXi’an Jiaotong University

In this work, diamond vertical Schottky barrier diodes (SBDs) with anodic self-aligned mesa termination were proposed and investigated. This kind of termination structure can effectively alleviate the electric field crowding at the Schottky electrode edge to avoid premature breakdown of the SBD, thus achieving high reverse blocking voltage. The targeted device showed prominent diode properties with a specific on-resistance of 4.0 mΩ/cm−2 and an on/off ratio of 109. The maximum blocking voltage increased from 206 to 460 V after utilizing mesa termination. The reverse leakage current was maintained below 10−2 A/cm2 until breakdown occurs. The mesa termination structure was analyzed theoretically by Silvaco TCAD, whose profiles showed that electrical concentration appears at the diamond mesa sidewall, and the peak electric field strength becomes lower with increasing mesa depth. These results indicate a feasible way to modify the electric field distribution and enhance the breakdown voltage of the diamond SBD.

  1. 2018 - Optoelectronic diamond: Growth, properties, and photodetection applications [Crossref]
  2. 2020 - Diamond power devices: State of the art, modelling, figures of merit and future perspective [Crossref]
  3. 2021 - Surface transfer doping of diamond: A review [Crossref]
  4. 2013 - 1 Ω on-resistance diamond vertical-Schottky barrier diode operated at 250 °C [Crossref]
  5. 2025 - High-temperature performance of metal/n-Ga2O3/p-diamond heterojunction diode fabricated by ALD method [Crossref]
  6. 2018 - Recent advances in diamond power semiconductor devices [Crossref]
  7. 2012 - High temperature application of diamond power device [Crossref]
  8. 2007 - Ramp oxide termination structure using high-k dielectrics for high voltage diamond Schottky diodes [Crossref]
  9. 2022 - Breakdown voltage enhancement of vertical diamond Schottky barrier diode with annealing method and AlO field plate structure [Crossref]
  10. 2018 - Electric field distribution using floating metal guard rings edge-termination for Schottky diodes [Crossref]