Skip to content

GPa Pressure Imaging Using Nanodiamond Quantum Sensors

MetadataDetails
Publication Date2025-11-19
JournalJournal of the Physical Society of Japan
AuthorsRyotaro Suda, Kenshin Uriu, Kouki Yamamoto, Misaki Sasaki, Kento Sasaki
InstitutionsOsaka University of Economics, The University of Tokyo
Citations4
AnalysisFull AI Review Included

Nanodiamond Quantum Sensing for High-Pressure Imaging: Technical Analysis

Section titled “Nanodiamond Quantum Sensing for High-Pressure Imaging: Technical Analysis”
  • Demonstration Platform: Wide-field optical microscopy of pressure distribution at ~20 GPa inside a diamond anvil cell (DAC) using nitrogen-vacancy (NV) centers hosted in 50 nm nanodiamonds (NDs) as quantum sensors.
  • Core Method: Optically detected magnetic resonance (ODMR) spectroscopy combined with a five-parameter uniaxial stress Hamiltonian that captures both axial pressure (PZ) and transverse pressure (P⊥).
  • Quantitative Anisotropy Extraction: The anisotropy ratio λ = PZ / P⊥ is mapped spatially at the micrometer scale, enabling visualization of non-hydrostaticity in real DAC geometries.
  • Critical Finding: The PTM (pressure-transmitting medium) architecture drastically alters local stress. Single-layer NaCl causes λ ≈ 1.6-1.8; double-layer NaCl drives λ ≈ 1.2-1.5 and a near-perfect hydrostatic condition.
  • Validation: Ruby fluorescence cross-check (20.6 GPa vs. 20.0 GPa) confirms the quantum sensing readout, establishing NV-ND ensembles as a calibrated nanoscale manometer.
  • Extendability: The same hardware stack is directly transferable to magnetic field imaging (e.g., iron under pressure) and superconducting transition studies in hydrides and nickelates.
  • Engineering Impact: This technique eliminates key limitations of ruby/Raman-based pressure metrology under non-hydrostatic conditions, where conventional techniques are unreliable.
ParameterValueUnitContext
Target Pressure Window~14-30GPaOperational range demonstrated (single-layer, 20.6 GPa ruby calibration)
Hydrostatic Equivalent Pressure~18.5GPaDouble-layer PTM, representative ODMR fit
Axial Pressure (PZ)14-30GPaSingle-layer PTM, distributed across chamber
Transverse Pressure (P⊥)10-20GPaSingle-layer PTM, distributed across chamber
Anisotropy Ratio (λ = PZ / P⊥)1.6-1.8 (center) / ~1.4 (edges)-Single-layer PTM
Anisotropy Ratio (λ = PZ / P⊥)1.2-1.5-Double-layer PTM (fitted with uniaxial model)
Hydrostatic Pressure Range17-20GPaDouble-layer PTM, full chamber
Zero-Field Splitting (Dgs)2.87GHzNV ground state at ambient pressure
ODMR Linewidth (single NV)12MHzModel parameter, hydrostatic simulation
ODMR Linewidth (ND ensemble)40-200MHzExperimental, depends on ensemble & pressure
ODMR Amplitude (C)0.0006-0.02-Simulated conditions
Pressure Coefficient (α₁)8.6MHz/GPaNV spin-stress coupling
Pressure Coefficient (α₂)−1.95MHz/GPaNV spin-stress coupling
Pressure Coefficient (β₁)−2.5MHz/GPaNV spin-stress coupling
Pressure Coefficient (β₂)−4.5MHz/GPaNV spin-stress coupling
Hydrostatic Pressure Shift (Πz)14.7MHz/GPaEquivalent linear shift coefficient
Laser Wavelength532nmCW excitation source
Optical Filters532 nm notch, 650 nm long-pass, 800 nm short-pass-Fluorescence isolation stack
Imaging Spatial Resolution~1µmWide-field microscopy via CMOS
Anvil Culet Diameter260µmDiamond anvil on the DAC
Gasket MaterialRhenium (Re)-Pre-indented to 42 µm from 250 µm
Sample Chamber Diameter100µmLaser-drilled
Sample (Iron) Dimensions~10 µm thickµm4N purity, Nilaco Co.
Ruby Crystal Size~10µmPressure calibration
ND Size50nmAdamas Nanotechnologies NDNV50nmHi10ml
Microwave AntennaFR4 (0.3 mm), Cu foil (18 µm)-Microstrip line with aperture, broadband
Operating TemperatureRoom (~25)°CNo external magnetic field
Microwave Frequency Range~2.87-3.45GHzODMR sweep window
  1. Sample Preparation (Single-Layer PTM)
    • Load NaCl powder at the bottom of the DAC chamber.
    • Place ruby crystal and iron sample on top of NaCl.
    • Place 50 nm NDs above sample, in direct contact with the upper diamond anvil.
    • Achieve ~20.6 GPa (ruby calibration).
  2. Sample Preparation (Double-Layer PTM)
    • Load NaCl powder at the bottom.
    • Place ruby, iron, and then ND layer.
    • Cap with a second NaCl layer to fully encapsulate the NDs, isolating them from the anvil culet.
    • Achieve ~20.0 GPa (ruby calibration).
  3. Wide-Field ODMR Imaging
    • Illuminate with a 532 nm CW laser through a high-NA objective.
    • Collect NV red photoluminescence (650-800 nm window) onto a CMOS camera.
    • Sweep microwave frequency via a custom microstrip-line antenna (FR4 / Cu).
  4. Data Acquisition
    • Acquire ODMR spectra pixel-by-pixel across the 100 µm chamber.
    • Apply pixel-level Lorentzian fits to extract local PZ, P⊥, and λ.
  5. Modeling & Fitting
    • Hydrostatic model: 3 parameters (C, Δν, P).
    • Uniaxial stress model: 5 parameters (C, Δν, PZ, P⊥, δ offset).
    • Includes orientation averaging (θ, ϕ, ψ), collection anisotropy A(θ, θmax), absorption efficiency κ(θ, ϕ), and quadratic microwave weighting factor M.
  6. Calibration Cross-Check
    • Validate by independent ruby fluorescence (±0.5 GPa agreement).
  7. Spectral Analysis
    • Exclude ambient-pressure ND contributions near 2.87 GHz from the fitting data.
Component in PaperRecommended 6CCVD MaterialRelevant Specification
Diamond Anvils (260 µm culet, high-pressure optical access)Optical-Grade Single Crystal Diamond (SCD)Plates/wafers up to 125 mm, Ra < 1 nm polish, low-birefringence
Nanodiamond Hosts (50 nm, NV ensembles)Custom NV-enriched ND slurry or BD/PCD NanopowderHigh-pressure-resistant, narrow size distribution for uniform ODMR
Future Magnetic Field Imaging TargetsBoron-Doped SCD (BDD) for conductive qubit-grade substrates—
Dense Cullet SubstratesPolycrystalline Diamond (PCD)Thickness 0.1-500 µm, custom-cut culet geometries
  • Diamond Anvil Engineering: The paper relies on a 260 µm culet anvil with a rhenium gasket pre-indented to 42 µm. 6CCVD can fabricate matching SCD cylinders and provide custom laser-cut culet geometries, including non-standard tip profiles for specialized DAC research.
  • Metalization: Microwave antenna integration (FR4-Cu microstrip line) would benefit from 6CCVD’s in-house metalization capabilities (Ti, W, Cu, Au, Pt, Pd) for patterning directly on diamond substrates or for matching impedance layers on gasket backing plates.
  • Laser Cutting & Dicing: Custom NV-ND deposition patterns on SCD, gasket machining, and patterned microfluidic-style sample chambers can be delivered via our laser cutting service.
  • Thickness Control: Polished SCD ranging from 0.1 µm to 500 µm allows for thin anvil slides or unusual spacer configurations if the chamber geometry must be adapted.
  • ODMR / Quantum Sensing Expertise: 6CCVD’s in-house PhD team can assist with material selection for NV-ND quantum sensing platforms, including recommendations on nitrogen concentration, NV yield, and surface functionalization to ensure reproducible ODMR contrast under high-pressure conditions.
  • Non-Hydrostatic Pressure Applications: We can support material choice when replicating the PTM study by providing NV-rich NDs suitable for DAC loading, characterized for size, purity, and fluorescence properties.
  • Anvil and Substrate Sourcing: Whether you need ultra-low-roughness SCD (Ra < 1 nm) for transmission optics or heavily boron-doped PCD for combined electrical/quantum readouts, 6CCVD provides a unified supply chain.

For custom specifications — including NV-doped nanodiamonds, optical-grade SCD anvils, or metallized diamond substrates tailored to your high-pressure quantum sensing, superconducting, or magnetic imaging program — visit 6ccvd.com or contact our engineering team directly.

View Original Abstract

We demonstrate wide-field optical microscopy of the pressure distribution at approximately 20 GPa in a diamond anvil cell (DAC), using nitrogen-vacancy (NV) centers in nanodiamonds (NDs) as quantum sensors. Pressure and non-hydrostaticity maps are obtained by fitting optically detected magnetic resonance (ODMR) spectra with models incorporating hydrostatic and uniaxial stress conditions. Two methods for introducing NDs with a pressure-transmitting medium are compared, revealing that the embedding approach affects the degree of non-hydrostaticity. This ND-based technique offers a powerful imaging platform for probing pressure-induced phenomena and is extendable to other physical quantities such as magnetic fields.