Fiber-integrated NV magnetometer with a microcontroller-based software lock-in technique
At a Glance
Section titled “At a Glance”| Metadata | Details |
|---|---|
| Publication Date | 2026-01-01 |
| Journal | Chinese Optics Letters |
| Authors | Qilong Wu, Xuan-Ming Shen, Yuan Zhang, Huihui Yu, Jinghao Zhang |
| Analysis | Full AI Review Included |
Executive Summary
Section titled “Executive Summary”- Miniaturized Quantum Sensing: Demonstration of a fiber-integrated NV magnetometer using a microcontroller (STM32F103ZET6) to replace bulky lock-in amplifiers and commercial microwave sources.
- Novel Software Lock-in Technique: Implementation of frequency-modulated (FM) ODMR entirely through firmware, eliminating the need for FPGA-based hardware lock-in systems.
- High Sensitivity at Low Cost: Achieved a magnetic field sensitivity of 93 nT/√Hz, comparable to commercial setups (421 nT/√Hz) at a fraction of the cost.
- Real-Time Field Tracking: Demonstrated real-time detection of a 1 Hz modulated magnetic field (0-0.2 mT range) with a standard deviation of 488 nT.
- Flexible Modulation Depth: Arbitrary modulation depth (up to 30 MHz), only limited by the microwave source chip (ADF4351) bandwidth, overcoming the 1 MHz limit of commercial signal generators.
- Compact Sensing Head: Microdiamond (40 µm, 3.5 ppm NV) attached to a 105 µm core multimode fiber, wrapped with a 150 µm copper coil antenna, all housed in a 300 µm capillary.
- Industrial Scalability: Validates the path toward credit-card-sized, portable NV magnetometers for EV charging monitoring, NDT, biomedical imaging, and high-voltage current sensing.
Technical Specifications
Section titled “Technical Specifications”| Parameter | Value | Unit | Context |
|---|---|---|---|
| Diamond Size | 40 | µm | Microdiamond sensing element |
| NV Concentration | 3.5 | ppm | Nitrogen-vacancy center density |
| Fiber Core Diameter | 105 | µm | Multimode optical fiber |
| Laser Wavelength | 520 | nm | Green laser excitation |
| Laser Power (max) | 130 | mW | Optical excitation source |
| Laser Power (operating) | 80 | mW | ODMR measurement condition |
| Microwave Power | 25 | dBm | Delivered to sensing head |
| Microwave Antenna Diameter | 150 | µm | Copper wire coil |
| Capillary Internal Diameter | 300 | µm | Protective housing |
| Fiber Coupling Efficiency | 90 | % | Optical-fiber coupler (FAC2-532-PC) |
| Magnetic Sensitivity (best) | 93 | nT/√Hz | At optimal modulation depth (13 MHz) |
| Magnetic Sensitivity (PSD avg) | 146 | nT/√Hz | Averaged over detection bandwidth |
| Electronic Noise Floor | 38 | nT/√Hz | Laser and microwave switched off |
| Off-Resonance Sensitivity | 115 | nT/√Hz | Frequency insensitive baseline |
| Detection Bandwidth | 40 | Hz | Configurable via sampling time |
| Max Detection Bandwidth | 2000 | Hz | Limited by ADF4351 switching speed |
| Modulation Depth Range | 1-30 | MHz | Software-configurable FM depth |
| Optimal Modulation Depth | 13 | MHz | Maximum slope (S = 15.5 mV/MHz) |
| Zero-Crossing Slope (S) | 16 | mV/MHz | At 2.91 GHz resonant feature |
| Real-Time Resolution | 488 | nT | Std. deviation over 1 s |
| ADC Resolution | 12 | bit | Integrated in microcontroller |
| External Amplification | 22× | - | TL082 op-amp gain for PD signal |
| Gyromagnetic Ratio (γ) | 2.8 | MHz/Gauss | NV center Zeeman coefficient |
| Microwave Frequency Range | 35-4400 | MHz | ADF4351 output capability |
| Microwave Attenuation Range | -30 to 0 | dB | HMC624A digital attenuator |
| Microwave Amplification | up to 40 | dB | KDT0308B-004 amplifier |
Key Methodologies
Section titled “Key Methodologies”-
Sensing Head Fabrication:
- Cleave multimode fiber (105 µm core) to produce flat facet.
- Pick single 40 µm microdiamond (3.5 ppm NV) with UV-curable adhesive.
- UV cure for 5 minutes to fix diamond.
- Insert fiber into 300 µm capillary; wind 150 µm copper wire as microwave antenna.
- Solder antenna to coaxial cable; connect to optical-fiber coupler.
-
Electronic Module Assembly:
- Microcontroller (STM32F103ZET6) coordinates via SPI protocol.
- Microwave source chip (ADF4351) provides radiation (35-4400 MHz).
- Digital attenuator (HMC624A) controls power; amplifier (KDT0308B-004) boosts signal.
- Voltage-controlled constant current source (KW-VCCS1000) drives 520 nm laser diode.
- Integrated 12-bit ADC samples photodetector (PDA36A2) output.
-
Optical Module Configuration:
- 520 nm laser reflected by dichroic mirror (OFD1LP-650).
- Coupled into multimode fiber via FAC2-532-PC coupler (90% efficiency).
- Fluorescence collected through same fiber, filtered by 650 nm LP filter (OFE1LP-650).
- Focused onto PD via convex lens (OLC220136).
- All components mounted on 3D-printed optical board.
-
Software Lock-in Technique:
- Switch microwave between two frequencies: δ₁ and δ₂.
- Center frequency: δc = (δ₁ + δ₂)/2; Modulation depth: δm = |δ₁ - δ₂|.
- ADC samples two voltage series {V₁}, {V₂} mimicking phase-locking.
- Compute averaged voltages Ṽ₁, Ṽ₂ and difference V_L = Ṽ₂ - Ṽ₁.
- Detection bandwidth tuned by varying voltage sampling time.
-
FM ODMR Measurement:
- Sweep carrier frequency across NV resonances (~2.87 GHz at zero field).
- Record lock-in voltage vs. carrier frequency.
- Fit spectrum using Lorentzian derivative model.
- Extract slope S at zero-crossing for magnetic field calibration.
-
Sensitivity Optimization:
- Vary modulation depth (δm) from 1 MHz to 30 MHz.
- Monitor lock-in voltage C₃, linewidth v₃, and slope S₃.
- Identify optimal δm = 13 MHz (S₃ maximum = 15.5 mV/MHz).
- Compute theoretical sensitivity: η = σ_L / (γS).
-
Real-Time Magnetic Field Detection:
- Place electromagnet below sensing head; modulate current at 1 Hz.
- Amplify PD signal 22× with TL082 op-amp.
- Set carrier frequency at zero-crossing point.
- Track lock-in voltage for continuous field readout.
6CCVD Solutions & Capabilities
Section titled “6CCVD Solutions & Capabilities”Applicable Materials
Section titled “Applicable Materials”This research requires precisely engineered diamond micro-particles with controlled NV center density. 6CCVD provides the following solutions:
| 6CCVD Material | Relevance to This Research |
|---|---|
| Single Crystal Diamond (SCD) Micro/Macro Particles | Replicate the 40 µm microdiamond sensing element. Custom sizes from 10 µm to bulk substrates available. |
| NV-Doped SCD (Engineered) | Controlled nitrogen incorporation (0.5-100 ppm range) to match the 3.5 ppm NV concentration used here. Optimized for ODMR coherence. |
| Optical-Grade SCD Wafers | Alternative for sensing heads requiring larger flat surfaces or thinner films (down to 0.1 µm). |
| Polycrystalline Diamond (PCD) | Cost-effective alternative for high-volume industrial magnetometer arrays. |
Recommended Specification for Replication:
- SCD particles, 40 µm ± 2 µm size distribution
- NV⁻ concentration: 3.5 ppm (customizable from 0.1-100 ppm)
- Surface roughness: Ra < 1 nm for optimal fluorescence collection
- Optional: Silver or Al coating for enhanced excitation/collection efficiency (as suggested in the paper’s future improvements)
Customization Potential
Section titled “Customization Potential”The paper identifies several optimization pathways that align with 6CCVD’s capabilities:
-
Precision Diamond Sizing: The authors explicitly state that replacing the 40 µm diamond with one matching the 105 µm fiber core would improve sensitivity by ~10×. 6CCVD offers custom particle sizing via laser cutting and precision lapping services.
-
Metallization for Sensing Heads: The copper wire antenna in this paper could be integrated directly onto diamond substrates. 6CCVD provides in-house metalization with Ti, Pt, Au, Pd, W, and Cu—all compatible with diamond substrates and microwave antenna patterning.
-
Microwave Antenna Integration: For next-generation sensing heads with on-diamond antennas or microstrip resonators, 6CCVD can deliver patterned metallization on SCD/PCD substrates.
-
Optical Coatings: The paper suggests silver-layer coatings or microconcave mirrors to enhance fluorescence. 6CCVD can supply diamond substrates with custom optical coatings and surface engineering (Ra < 1 nm SCD polish standard).
-
Substrate Geometries: For credit-card-sized board integration, 6CCVD offers SCD/PCD plates and wafers up to 125 mm diameter with thickness from 0.1 µm to 500 µm.
Engineering Support
Section titled “Engineering Support”6CCVD’s in-house PhD engineering team specializes in diamond materials for quantum sensing applications. We provide:
- Material Selection Consultation: Guidance on SCD vs. PCD, nitrogen concentration targets, and isotope purification (¹²C enrichment) for extended coherence times.
- Prototype-to-Production Scaling: From single research-grade microdiamonds to batch-produced sensor arrays.
- Custom Geometry Fabrication: Non-standard shapes, thin membranes, and patterned substrates for MEMS-integrated magnetometers.
- Metallization Design Support: RF-compatible electrode patterns for microwave delivery and spin manipulation.
Application Alignment
Section titled “Application Alignment”This research directly supports deployment in:
- Electric Vehicle Charging Detection: Real-time current monitoring via magnetic field sensing.
- Industrial NDT: Non-destructive testing of ferromagnetic materials.
- Biomedical Imaging: Magnetocardiography and cell-tracking applications.
- High-Voltage Current Monitoring: Grid infrastructure and power electronics.
Call to Action
Section titled “Call to Action”For custom specifications or material consultation on NV magnetometer diamond components, visit 6ccvd.com or contact our engineering team directly.
Reference: Wu et al., “Fiber-integrated NV Magnetometer with Microcontroller-based Software Lock-in Technique,” Zhengzhou University, 2025.
View Original Abstract
Fiber-integrated nitrogen-vacancy (NV) magnetometers possess high sensitivity, integration, and flexibility, and thus have been explored extensively for industrial applications. While most studies have focused on the optimization of the quantum sensing head, less attention has been paid to the frequently employed professional, expensive, and bulky electronics, which hinder their practical applications. In this article, we fabricate a fiber-integrated NV magnetometer and develop a low-cost microcontroller-based software lock-in technique. In this technique, a microcontroller coordinates efficiently a microwave source chip and an analog-to-digital converter, and a program mimicking the lock-in mechanism realizes microwave frequency-modulated optically detected magnetic resonance of NV centers. As a result, with our setup and technique, we have realized the detection of weak magnetic field with a sensitivity of 93 nT/Hz^{1/2}, which is comparable to what obtained with bulky and professional devices. Furthermore, we demonstrated real-time magnetic field detection, achieving a standard deviation of 488 nT. Our work provides a novel and cost-effective technique for electronic miniaturization, thereby potentially accelerating the industrial application of NV magnetometers.
Tech Support
Section titled “Tech Support”Original Source
Section titled “Original Source”References
Section titled “References”- 2020 - Sensitivity optimization for NV-diamond magnetometry [Crossref]
- 2024 - Single-molecule scale magnetic resonance spectroscopy using quantum diamond sensors [Crossref]
- 2021 - Quantum guidelines for solid-state spin defects [Crossref]
- 2013 - Solid-state electronic spin coherence time approaching one second [Crossref]
- 2025 - Solid-state spin coherence time approaching the physical limit [Crossref]
- 2014 - Quantum error correction in a solid-state hybrid spin register [Crossref]
- 2014 - Universal control and error correction in multi-qubit spin registers in diamond [Crossref]
- 2017 - Entanglement distillation between solid-state quantum network nodes [Crossref]
- 2017 - Quantum sensing [Crossref]